Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |
50*50*40(mm)
Panel size available:
1788*4531,1225*5035 Bidirectional force.
Bearing bar thickness (Top/Bottom):6.8/5.0
Bearing bar center:50
Open Aera:80%
Approx Weight:15.82kgs/m²
Liner load(units:mm)
Span in (mm) | Load in kn/m of widht (concentrated) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
|---|---|---|---|
| 400 | 4.4 | 30 | 11.8 |
| 600 | 11.8 | 21 | 14.9 |
Uniform load(units:mm)
Span in (mm) | Load in kn/sqm (uniformed) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
|---|---|---|---|
| 400 | 1.1 | 154 | 11.8 |
| 600 | 4.4 | 73 | 14.9 |
| 800 | 1.3 | 35 | 16.6 |
The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
FRP molded grating 50*50 H40 is commonly used for working platforms, walkways, trench covers, stair treads and equipment operating surfaces that require slip resistance, corrosion resistance and load-bearing capacity. Its 50 mm mesh and 40 mm height suit applications needing open drainage, ventilation or reduced self-weight. For suitability under specific working conditions, please contact us to evaluate together with site conditions.
Selection Guide
During selection, first clarify load-bearing requirements, span, corrosive media and fire protection requirements, then determine the resin system, grating thickness and mesh size accordingly. Different resin types have different emphases in chemical resistance and flame retardant performance, and need to match the service environment. Please contact us for detailed specifications and selection advice.
Product Advantages
Molded grating is formed as a whole, with fibers and resin evenly distributed. It combines light weight, high strength, corrosion resistance and two-way load-bearing characteristics, with a slip-resistant surface that is easy to cut and install. Compared with traditional metal grating, it is more suitable for humid, acid-base or salt-spray environments. For specific performance details, please contact us for more information.
Inquiry Guide
To confirm whether FRP molded grating 50*50 H40 is suitable for your project, please provide the service environment, load-bearing requirements and size requirements, and we will help match a solution. Please contact us for detailed specifications and a quotation.
Operating Environment
- This molded FRP grating (50×50 mm mesh, 40 mm depth) is built from unsaturated polyester resin, so it suits both indoor and outdoor installations where moisture and weather exposure are present.
- The corrosion-resistant resin skeleton makes it suitable for service around the chemical, wastewater and process-plant areas where aggressive media would attack metal gratings.
- With the phenolic-type resin option offering high flame-retardant performance and low toxicity, this grating can be used in areas where fire safety is a concern.
- Its E-glass fiber reinforcement keeps the panel stable under humid and varying outdoor conditions; contact us for the full parameter list for your specific environment.