Product Category

玻璃钢模塑格栅40*40H30


Contact us for a quotation

产品详情

Genius FRP    

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---


Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber    

Code

Coarse sand type

Recommended usage occasion

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasion

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Groove type

Polished type

Shop sand type

40*40*30(mm)

Panel size available:

1247*4047,1007*4047,1007*3007 

Bidirectional force.

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:40

Open Aera:67%

Approx Weight:14.6kgs/m²

Liner load(units:mm)

Deflcvtion

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

Span( mm)

751503004507501500

Load

300<0.25<0.250.260.510.761.539924
4500.260.511.021.532.543.924828
6000.511.272.293.565.857.384113
7501.272.544.837.3712.5163174
9002.274.549.0813.718.822.12638

Uniform load(units:mm)

Deflcvtion

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Span( mm)

350500750100015002500
3000.290.480.570.751.151.82
4500.781.191.812.473.545
6001.762.664.285.568.4113.2
7503.485.128.211116.5---
9005.898.8114.219------

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

 

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  


Application Scenarios

FRP molded grating 40*40 H30 is widely used in operating platforms, walkways, stair treads and trench covers in petrochemical, power, wastewater treatment, marine engineering and other fields. Its corrosion resistance, slip resistance, light weight and high strength make it suitable for humid, acid and alkali corrosive environments. To learn about its applicability under specific working conditions, please contact us for detailed specifications and quotations.

Selection Guide

Selection requires comprehensive consideration of load-bearing requirements, span, corrosive environment and safety needs. Different resin types (such as orthophthalic, isophthalic, vinyl ester and bisphenol A) and thicknesses affect the grating's corrosion resistance, flame retardancy and mechanical properties. It is recommended to choose a suitable model based on actual usage conditions. Please contact us for detailed specifications and quotations.

Product Advantages

FRP molded grating features excellent corrosion resistance, light weight, high strength, slip resistance, insulation and long service life. Its surface groove or grit design provides good anti-slip performance, and it is easy to cut and install with low maintenance costs. To learn about specific performance data, please contact us for detailed specifications and quotations.

Inquiry Guidance

If you are interested in FRP molded grating 40*40 H30 or have specific requirements, please contact us for detailed specifications and quotations. We can provide customized solutions to meet your project requirements.

Operating Environment

  • Molded FRP grating (40×40H30) is based on unsaturated polyester resin, with resin type selectable for specific chemical exposure.
  • Intended for industrial settings, including indoor and outdoor platforms, walkways, and stair treads.
  • Service conditions such as temperature, humidity, and corrosive media should be matched to the selected resin grade.
  • For environments with fire safety requirements, phenolic resin options are available with flame retardant properties.