Product Category

玻璃钢模塑格栅38*38H60重负载型


Contact us for a quotation

产品详情

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.  

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Groove type

Polished type

Shop sand type

38*38*60(mm)

Panel size available:

1220*4000,1220*3660,1220*2440,

915*3050 Bidirectional force.

Bearing bar thickness (Top/Bottom):11.5/9.0

Bearing bar center:38.1mm( 1.5")

Open Aera:54%

Approx Weight:50.4kgs/m²

Liner load(units:mm)

Span in (mm)

Load in kn/m of widht (concentrated)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

40011.2197.14

Uniform load(units:mm)

Span in (mm)

Load in kn/sqm (uniformed)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

4002.81007.14
60011.8458.55

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in: 

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  


Application Scenarios

This product is a heavy-duty FRP molded grating with a 38×38 mm mesh and 60 mm thickness, suitable for industrial platforms, walkways, trench covers and corrosive environments such as chemical, wastewater treatment and marine engineering that require high load capacity and corrosion resistance. If your operating conditions involve strong acids or alkalis, humidity or long-term outdoor exposure, please contact us with your service conditions for tailored recommendations.

Selection Guide

When selecting, please focus on load requirements, span, support method and the type of corrosive medium, and match these with the resin system (such as orthophthalic, isophthalic, vinyl ester, bisphenol A, etc.) and anti-slip surface requirements. As requirements for thickness, mesh size and resin selection vary greatly between operating conditions, please provide drawings or process parameters and we will help confirm suitable specifications.

Product Advantages

FRP molded grating is integrally molded from unsaturated polyester resin and glass fiber, combining light weight, high strength, corrosion resistance, anti-slip and insulation properties, and is easy to cut, install and maintain. The 38×38 mm mesh and 60 mm thickness design provides high load capacity while maintaining ventilation and light transmission, making it suitable for heavy-duty applications.

Inquiry Guide

For detailed specifications, resin options, colors, surface treatments and packaging of this product, please contact us for full specifications and a quotation. Please provide your application environment, load requirements and dimensional needs, and we will recommend a suitable solution and respond with commercial terms as soon as possible.