Product Category

FRP Molded Grating 38×38 H60 Heavy-Duty Type


Contact us for a quotation

Product details

Greenlogy TEC

FRP molded grating is a panel with a certain open area, made in custom molds with unsaturated polyester resin (including isophthalic, orthophthalic, phenolic and bisphenol types) as the matrix. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Glass fiber

33%

E

Filler

31%

ATH,PR

Other

1%

---

Introduction to raw materials

Resin type

Code

Resin type

Flame retardancy

Recommended applications

MP-5

Phenolic type

Oxygen index up to about 80

Low toxicity and high flame retardancy, suitable for applications with high fire safety requirements

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

VEFR-10

Vinyl ester type

Oxygen index above 35

Applications with high acid and alkali resistance and high flame retardancy requirements

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR economical type, good performance, resistant to moderate acids, alkalis and solvents

IFGR-30

Styrene-based food grade

Oxygen index 26

Mainly used for meat products and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical type, no flame-retardant requirement

Coarse fiberglass selection

Code

Coarse grit type

Recommended applications

E

Alkali-free (E-glass) grit

For high-strength requirements and highly corrosion-resistant applications

Selected filler type

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing, corrosion-resistant applications

PR

No filler, pure resin

For highly corrosion-resistant applications

Channel section

Polished type

Workshop sand mold

38*38*60(mm)

Optional panel sizes:

1220*4000,1220*3660,1220*2440,

915*3050 Bi-directional load bearing.

Bearing flat bar thickness (top/bottom): 11.5/9.0

Bearing flat bar center distance: 38.1mm (1.5")

Open area: 54%

Approximate weight: 50.4kgs/m²

Linear load (unit: mm)

Span (mm)

Load in width direction (kN/m, concentrated load)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

40011.2197.14

Uniform load (unit: mm)

Span (mm)

Load kN/sqm (uniform)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

4002.81007.14
60011.8458.55

Features:

  1. Corrosion resistant

  2. Slip resistant

  3. Excellent ergonomic design

  4. Low installation cost

  5. Flame retardant

  6. Lightweight with high bi-directional strength; cutting makes the pipe easier to install.

  7. Uniform color inside and out; colors can be selected freely.

  8. Delivers good social and economic benefits.

  9. Flexible design, diverse sizes, and dimensional stability

Widely used in:

Greenlogy TEC FRP grating is widely used for industrial platform floors, stairs, walkways and platforms. Using FRP grating offers many advantages: good weather resistance, low maintenance costs, long service life and good slip resistance. In addition, FRP grating is simple, fast and flexible to fabricate and assemble.


Application Scenarios

This product is a heavy-duty molded FRP grating with a 38×38mm mesh and 60mm thickness, suitable for industrial platforms, walkways, trench covers and corrosive environments such as chemical, wastewater treatment and marine engineering that require high load capacity and corrosion resistance. If your operating conditions involve strong acids or alkalis, humidity or long-term outdoor exposure, please contact us with your service conditions for suitable recommendations.

Selection Guide

When selecting, please focus on load requirements, span, support method and the type of corrosive medium, and match these with the resin system (such as orthophthalic, isophthalic, vinyl ester, bisphenol A, etc.) and surface slip-resistance requirements. Since different operating conditions vary considerably in thickness, mesh size and resin selection, please provide drawings or operating parameters and we will help confirm the appropriate specification.

Product Advantages

Molded FRP grating is integrally molded from unsaturated polyester resin and glass fiber, combining light weight, high strength, corrosion resistance, slip resistance and electrical insulation, and is easy to cut, install and maintain. The 38×38mm mesh and 60mm thickness design provides high load capacity while maintaining ventilation and light transmission, making it suitable for heavy-duty applications.

Inquiry Guidance

For detailed specifications, resin options, colors, surface treatments and packaging of this product, please contact us for detailed specifications and a quotation. Please provide your application environment, load requirements and size requirements, and we will recommend a suitable solution and reply with commercial terms as soon as possible.