产品详情
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property |
Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |
38*38*50(mm)
Panel size available:
1220*4000,1220*3660,1220*2440,
915*3050 Bidirectional force.
Bearing bar thickness (Top/Bottom):11/9.0
Bearing bar center:38
Open Aera:56%
Approx Weight:42kgs/m²
Liner load(units:mm)
Span in (mm) |
Load in kn/m of widht (concentrated) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
| 400 | 9.3 | 19 | 7.14 |
Uniform load(units:mm)
Span in (mm) |
Load in kn/sqm (uniformed) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
|---|---|---|---|
| 400 | 2.3 | 100 | 7.14 |
| 600 | 9.9 | 45 | 8.55 |
The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
Greenlogy TEC FRP molded grating 38*38 H50 heavy-duty type is suitable for operating platforms, walkways, trench covers and other applications requiring high load-bearing capacity and corrosion resistance in petrochemical, power, wastewater treatment, marine engineering and other industries.
Its 38*38mm mesh and 50mm thickness design provides high strength while maintaining drainage, anti-slip and ventilation performance, making it suitable for humid environments, areas prone to liquid accumulation, or places requiring frequent washing.
Selection Guide
When selecting, load-bearing requirements, span, support method and service environment should be comprehensively considered, and appropriate thickness and mesh size should be selected according to actual loads.
If a higher corrosion resistance grade is required, isophthalic, vinyl ester or bisphenol A resins can be selected; when flame retardant performance is needed, formulations with added flame retardants are available. Please contact us for detailed specifications and selection advice.
Product Advantages
This product uses unsaturated polyester resin as the matrix and is reinforced with glass fiber, featuring lightweight and high strength, corrosion resistance, aging resistance, insulation and maintenance-free properties.
The molding process ensures accurate mesh dimensions and good integrity, the surface groove design provides anti-slip effect, and the heavy-duty structure can withstand relatively large concentrated loads.
Inquiry Guide
For more information on the technical parameters, customized sizes or bulk purchase of Greenlogy TEC FRP molded grating 38*38 H50 heavy-duty type, please contact us for detailed specifications and quotations.
We can provide selection support and solutions according to your specific needs. Please feel free to contact us.
Operating Environment
- Molded FRP grating with 38×38 mm mesh and 50 mm depth is built for heavy-load service in industrial plants, walkways, platforms and stair treads where steel grating would corrode.
- The isophthalic, vinyl ester and bisphenol unsaturated polyester resin systems named in the raw-material table suit outdoor and indoor exposure to moisture, humidity and chemical splash; the phenolic grade is offered where fire safety and low toxicity are required.
- Because the load-bearing structure is molded from resin, E-glass fiber and ATH or PR filler rather than welded metal, the grating performs in corrosive and wet atmospheres where periodic washdown is normal.
- For temperature limits, chemical resistance ratings against specific media and the full parameter list, contact Greenlogy TEC with your service conditions.