Product Category

玻璃钢模塑格栅38*38H25


Contact us for a quotation

产品详情

Genius FRP

    Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

            Introduction of raw materials

            Resin type  

            Code

            Resin type

            Flame retardant property

            Recommended usage occasions

            MP-5

            Phenolic type

            Oxygen index can reach about 80

            Low toxicity and high flame retardant, fire safety is very important for the occasion

            VEFR-5

            Vinyl type

            Oxygen index 28 or above

            Acid, alkali and other corrosive harsh environment

            VEFR-10

            Vinyl type

            Oxygen index 35 or above

            Flame retardant requirements of high acid, alkali and good occasions

            IFR-25

            Meta benzene

            Oxygen index 28 or above

            A VEFR type economy, and excellent, moderate acid alkali and solvent

            IFGR-30

            Benzene food grade

            Oxygen index 26

            Mainly used in meat products and food processing plants

            OFR-25

            Ortho type

            Oxygen index 28 or above

            General acid and alkali environment

            OCR

            Ortho type

            Oxygen index below 28

            OFR-25 economy, no flame retardant requirements

            The type selection of coarse glass fiber   

            Code

            Coarse sand type

            Recommended usage occasions

            E

            Non alkali sand

            For high strength requirements and high corrosion resistance of the occasion

            Selected filler type    

            Code

            Filler type

            Recommended usage occasions

            ATH

            Aluminum hydroxide

            Retardant, smoke suppression, corrosion-resistant occasions

            PR

            No filler, pure resin

            For high corrosion-resistant applications

            Groove type

            Polished type

            Shop sand type

            38*38*25(mm)

            Panel size available:

            1220*4010,1220*3660,1524*4010,

            997*3012,915*3050Bidirectional force.

            Bearing bar thickness (Top/Bottom):6.4/5.0

            Bearing bar center:38

            Opea Area:68%

            Approx Weight:12.3kg/㎡

            Liner load(units:mm)

            Deflcvtion


             

            kg/m




            Limit

            Span
            (mm)
            75150300450600750Load
            450
            0.561.1563.074.114.753910
            6000.861.703.505.161 8.18 2924
            9002.905.9212.118.4   ---   --- 1948
            12005.72111    ---   ---   ---   ---  1461

            Uniform load(units:mm)

            Deflcvtion


             


            kg/m²



            Limit

            Span
            (mm)
            240480980145024503650Load
            450
            0.661.11.932.774.476.58---
            6001.122.14.146.1710.215.3   ---   
            7502.675.3910.816.3   ---   --- ---
            9005.5411.221.7   ---   ---   ---  ---

            The characteristics:

            1. Corrosion Resistant 

            2. Slip Resistant 

            3. Superior Ergonomics 

            4. Low Install Cost 

            5. Fire Retardant 

            6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

            7. The internal and external uniform color and color can be arbitrary choice.

            8. It has good social and economic benefits.

            9. Can design , flexible and varied size, size stability

             

            Widely used in:

               Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

             


             


            Application Scenarios

            FRP molded grating 38*38H25 is widely used for working platforms, walkways, stair treads and trench covers in chemical, petroleum, power, wastewater treatment, marine engineering and other fields. Its corrosion resistance, slip resistance and light weight make it an ideal choice for wet and corrosive environments.

            Selection Guide

            When selecting, please consider load requirements, corrosive environment, fire resistance requirements and installation method. Different resin types (such as orthophthalic, isophthalic, vinyl ester and bisphenol A) and additives (such as ATH and PR) can provide different corrosion resistance and flame-retardant performance. Please contact us for detailed specifications and selection advice.

            Product Advantages

            FRP molded grating offers excellent corrosion resistance, high strength, light weight, slip resistance, insulation and long service life. Its 38*38mm mesh and 25mm thickness design balances load bearing and open area, making it easy to install and maintain.

            Inquiry Guide

            For more information on the technical parameters, price and customization services of FRP molded grating 38*38H25, please contact us for detailed specifications and a quotation. Our professional team will help you select a suitable solution.

            Operating Environment

            • Molded FRP grating is suited to both indoor and outdoor installations, including platforms, walkways and stair treads in industrial plants, water treatment facilities and chemical processing areas.
            • The unsaturated polyester resin and glass fiber construction resists corrosion from acids, alkalis, salts and many other chemical media, making it suitable for wet, humid or splash-exposed locations.
            • With no metal content, the grating does not rust and requires no painting, so it performs in coastal and other environments where steel would deteriorate.