Greenlogy TEC

Fiberglass reinforced plastic (FRP) molded grating is a panel with a certain open area, made in a custom mold with unsaturated polyester resin (including isophthalic, orthophthalic, phenolic and bisphenol types) as the matrix.

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Glass fiber

33%

E

Filler

31%

ATH,PR

Other

1%

---

Raw material introduction

 Resin type  

Code

Resin type

Flame retardancy

Recommended applications

MP-5

Phenolic type

Oxygen index up to approximately 80

Low toxicity and high flame retardancy; fire safety is very important in these applications

VEFR-25

Vinylester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

VEFR-10

Vinylester type

Oxygen index 35 and above

Applications with high acid and alkali exposure and high flame-retardant requirements

IFR-25

Isophthalic type

Oxygen index 28 and above

A VEFR economical grade, with good performance and resistance to moderate acids, alkalis and solvents

IFGR-30

Benzene-based, food grade

Oxygen index 26

Mainly used for meat products and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical grade, no flame retardancy requirement

Chopped glass fiber selection  

Code

Chopped strand mat type

Recommended applications

E

E-glass

For high-strength requirements and high corrosion resistance applications

Filler type selection 

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame retardant, smoke suppression and corrosion resistance applications

PR

No filler, pure resin

For high corrosion resistance applications

Grooved type

Polished type

Workshop sand-surface type

38*152*38(mm)

Available panel sizes:

1220*3660, 1220*2440, 915*3050 lengthStress      

Load-bearing flat bar thickness (top/bottom): 8.0/6.0

Load-bearing flat bar center spacing: 38

Open area: 67%

Approximate weight: 15.92 kgs/m²

Line load (unit: mm)

Deflection

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Ultimate

Span (mm)

75150300450600750

Load

300<0.25<0.250.250.510.510.7612628
450<0.250.250.761.021.521.789946
6000.250.761.522.293.053.818233
7500.761.272.794.065.336.67040
9001.022.294.326.648.6410.96146
10501.523.36.69.91------5439
12002.294.839.65---------5141

Uniformly distributed load (unit: mm)

Deflection

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Ultimate

Span (mm)

350450750100015002500

Load

300<0.25<0.25<0.250.250.250.5141358
450<0.250.250.510.761.021.7826962
6000.511.021.271.782.794.5721716
7501.032.033.054.066.35---18446
9002.544.066.18.1312.2---13420
10504.577.1110.7---------10180
12007.8711.9------------8418

Features:

  1. Corrosion resistance 

  2. Slip resistance 

  3. Superior ergonomics 

  4. Low installation cost 

  5. Flame retardant 

  6. Lightweight, bidirectional strength, and easy cutting make the pipe easier to install.

  7. Uniform color inside and out; colors can be selected freely.

  8. Delivers favorable social and economic benefits.

  9. Designable, flexible and varied in size, with stable dimensions

Widely used in:

Greenlogy TECFRP grating is widely used for industrial platform floors, stairs, walkways and platforms. Using FRP grating offers many advantages: good weather resistance, low maintenance cost, long service life and good anti-slip performance. In addition, FRP grating is simple, fast and flexible to process and assemble.


Application Scenarios

FRP molded grating 38*152H38 is suitable for operating platforms, walkways, trench covers and stair treads in petrochemical, power, wastewater treatment and marine engineering fields. Its corrosion resistance, light weight and high strength deliver excellent performance in humid, acid and alkali corrosive environments.

Selection Guide

Selection should consider load requirements, service environment (corrosive media, temperature) and safety needs (such as flame retardancy and anti-slip). Different resin types (such as orthophthalic, isophthalic, vinyl ester and phenolic) provide different corrosion resistance and flame retardancy, and can be selected according to specific working conditions. Contact us for detailed specifications and selection advice.

Product Advantages

FRP molded grating offers advantages such as light weight and high strength, corrosion resistance, anti-slip performance, insulation and maintenance-free operation, and colors and sizes can be customized on request. Its unique mesh structure makes installation and cutting easy, suitable for various complex applications.

Inquiry Guide

For more product information, technical parameters or a quotation, please contact us at any time. We provide professional technical support and customization services, and welcome your inquiry.

Service Environment

  • Molded FRP grating 38*152H38 is suitable for outdoor and indoor service environments in industrial plants, and can replace steel grating where humidity and chemical corrosion shorten service life.
  • The isophthalic, vinyl ester and bisphenol A polyester resin systems specified above are suitable for continuous contact with acidic, alkaline and saline media in chemical, wastewater treatment and coastal facilities.
  • The E-glass fiberglass reinforcement and ATH / PR filler contents listed in the material table give molded grating dimensional stability under humid and wet conditions, along with rot resistance and corrosion resistance.
  • The phenolic resin grade (MP-5) in the raw material list is suitable for areas with low toxicity and high flame retardancy requirements, such as tunnels, offshore platforms and confined spaces where fire safety requirements are relatively high.