Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.  

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

 The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

 Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Groove type

Polished type

Shop sand type

19*19*38(mm)

Panel size available:

1524*4000,1220*3660,1220*2440,

915*3050 Bidirectional force.

Bearing bar thickness (Top/Bottom):7.5/5.0

Bearing bar center:19

Open Aera:40%

Approx Weight:23.5kgs/m²  

Liner load(units:mm)

Deflcvtion

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

Span( mm)

150

300

450

600

750

1500

Load

3000.360.480.610.760.891.0617116
6000.661.251.852.463.078.488718
9001.83.685.567.429.313.85817
12004.759.6814.619.621.2---3755

Uniform load(units:mm)

Deflcvtionkg/m²kg/m²kg/m²kg/m²kg/m²kg/m²kg/m²
Span(mm)2404809801450245036504880
3000.090.190.380.490.781.05---
6000.430.811.552.313.845.74---
9001.703.456.9610.517.523.3---
12005.9712.224.532.638.7------

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  


Application Scenarios

FRP molded grating 19*19H38 is suitable for walkways, platforms, trench covers and equipment operating surfaces that require slip resistance, corrosion resistance and load-bearing capacity. It is commonly used in humid or corrosive environments such as chemical, water treatment, electroplating and marine engineering. Different resin systems can be selected according to specific media and working conditions. Please contact us with your operating environment for matching recommendations.

Selection Guide

Selection can be considered from four dimensions: resin type, grating thickness, mesh size and load-bearing requirements. The corrosive medium determines the resin system, while span and load determine thickness and support method. As specific working condition parameters are involved, please contact us with your operating conditions so our technical staff can assist in confirming suitable specifications.

Product Advantages

Molded grating is integrally formed from resin and fiberglass, featuring light weight, high strength, corrosion resistance, slip resistance and insulation, and is easy to cut, install and maintain. Compared with traditional metal grating, it is less prone to rust in humid and corrosive environments, helping to reduce long-term maintenance costs.

Inquiry Guide

For detailed specifications, resin options, packaging methods and delivery arrangements of 19*19H38 molded grating, please contact us for detailed specifications and a quotation. Please provide your operating environment, required dimensions and quantity, and we will provide a targeted solution accordingly.