Greenlogy TEC
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |
19*19*25(mm)
Panel size available:
1220*4000,1220*3660,1220*2440,
915*3050 Bidirectional force.
Bearing bar thickness (Top/Bottom):6.5/5.0
Bearing bar center:19
Open Aera:40%
Approx Weight:16.8kgs/m²
The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
FRP Molded Grating 19*19H25 offers excellent corrosion resistance, slip resistance and load-bearing performance, making it suitable for operating platforms, walkways, drainage trench covers and stair treads in chemical, petroleum, power, wastewater treatment, marine engineering and other fields. Its lightweight and high-strength characteristics also make it easy to install and remove, ideal for locations requiring frequent maintenance.
Selection Guide
When selecting, consider load-bearing requirements, span, corrosivity of the service environment and flame-retardant grade. Different resin types (such as orthophthalic, isophthalic, vinyl ester and phenolic) correspond to different corrosion resistance and flame-retardant performance, so the appropriate resin system can be chosen according to specific working conditions. Please contact us for detailed specifications and selection advice.
Product Advantages
FRP molded grating is formed in a single molding process, with good structural integrity, high strength and light weight, only about 1/4 that of steel grating. Its surface has anti-slip protrusions, and anti-slip materials such as quartz sand can be added as required. The product resists corrosion from various chemical media, has a long service life and low maintenance cost, and offers good insulation and non-magnetic properties.
Inquiry Guide
For detailed specifications, prices and supply information of FRP Molded Grating 19*19H25, please contact us for professional consultation and quotation. We can provide customized solutions according to your specific needs.
Operating Environment
- Molded FRP grating with a 19×19 mm mesh and 25 mm depth is used in industrial plants, water treatment facilities and chemical processing areas where the working environment may be humid, wet or subject to occasional splashes.
- The unsaturated polyester resin matrix resists many corrosive media found in process industries, making the grating suitable for both indoor installations and outdoor platforms exposed to weather.
- With an oxygen index up to about 80 for phenolic-type resin, the grating is intended for locations where fire safety is a primary concern, such as areas with flammable materials or high-temperature processes.
- For detailed chemical resistance data, temperature limits and UV performance in your specific operating conditions, please contact us with your application details.