   FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.   

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

FL-A508*7*50.8*819.7

20" x 1/4" x 2" x 5/16"

43.4
FL-B635*12*101.6*1354.6

25" x 1/2" x 4" x 1/2"

120
FL-C498*4*50*49.4

20" x 3/16" x 2" x 3/16"

20.7

50*20*4*40.7

2" x 13/16" x 3/16" x 3/16"

1.54

55*31*3*30.6

9/4" x 5/4" x 1/8" x 1/8"

1.32

Markets  

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:    

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.    

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar  

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Isophthalic structural profile floor panels are suitable for industrial platforms, walkways, trench covers, and offshore facilities with high corrosion resistance requirements. Their lightweight, high-strength, and chemical-resistant properties make them widely used in chemical, marine, and wastewater treatment industries.

Selection Guide

Selection requires comprehensive consideration of load requirements, span, support spacing, and service environment. Profiles of different cross-sectional dimensions and thicknesses have varying load-bearing capacities. We recommend consulting our technical team based on actual engineering conditions to obtain suitable specification recommendations.

Product Advantages

The isophthalic resin system gives the floor panels excellent corrosion resistance and water resistance, while glass fiber reinforcement ensures high strength and stiffness. The products are lightweight for easy transportation and installation, and offer good insulation and aging resistance.

Inquiry Guide

For detailed specifications, technical parameters, or customized solutions, please contact us for professional support and quotations. We can provide selection advice and solutions based on your project requirements.

Operating Environment

  • These isophthalic resin FRP floor profiles are pultruded glass fiber composites intended for both indoor plant flooring and outdoor walkways, platforms and stair treads, where the profile replaces steel grating in wet or humid service.
  • The isophthalic resin matrix is chosen for resistance to mildly corrosive media - splash, salt-laden air and washdown conditions found in chemical, water treatment and marine-adjacent plants - rather than for concentrated acids or strong solvents.
  • Because the pultruded profile carries no steel core, it is suited to areas where corrosion of conventional metal grating would demand frequent recoating; the surface is non-sparking and does not support rust staining of surrounding structures.
  • Service temperature, chemical exposure and UV loading vary by installation; contact Greenlogy TEC with the actual service conditions so the appropriate resin grade, profile size from the FL-A / FL-B / FL-C range and fastening details can be confirmed.