Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.
Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Riglet | Width*Thickness | Width*Thickness |
| |
FS19 | 19*6.4 | 0.25 | 3/4" x 1/4" | 0.55 |
FS30A | 30*3 | 0.18 | 19/16" x 1/8" | 0.4 |
FS30B | 30*6.4 | 0.37 | 19/16" x 1/4" | 0.82 |
FS35 | 35*8 | 0.54 | 11/8" x 5/16" | 1.19 |
FS38 | 38*5 | 0.37 | 3/2" x 3/16" | 0.82 |
FS40A | 40*8 | 0.62 | 25/16" x 5/16" | 1.37 |
FS40B | 40*10 | 0.79 | 25/16" x 3/8" | 1.74 |
FS46B | 46*6.4 | 0.58 | 29/16" x 1/4" | 1.28 |
FS50A | 50*2 | 0.25 | 2" x 1/16" | 0.55 |
FS50B | 50*4 | 0.38 | 2" x 3/16" | 0.84 |
FS50C | 50*6 | 0.59 | 2" x 1/4" | 1.3 |
FS50D | 50*8 | 0.76 | 2" x 5/16" | 1.68 |
FS50E | 50*15 | 1.43 | 2" x 9/16" | 3.15 |
FS60A | 60*2 | 0.24 | 19/8" x 1/16" | 0.53 |
FS60B | 60*4 | 0.48 | 19/8" x 3/16" | 1.06 |
FS64 | 64*4.8 | 0.6 | 5/2" x 3/16" | 1.32 |
FS70 | 70*4 | 0.55 | 11/4" x 3/16" | 1.21 |
FS76 | 76*9.5 | 1.42 | 3" x 3/8" | 3.13 |
FS100A | 100*10 | 1.95 | 4" x 3/8" | 4.3 |
FS100B | 100*25 | 4.85 | 4" x 1" | 10.7 |
FS102A | 102*3.2 | 0.63 | 4" x 1/8" | 1.39 |
FS102B | 102*5 | 0.97 | 4" x 3/16" | 2.4 |
FS102C | 102*6.4 | 1.3 | 4" x 1/4" | 2.87 |
FS120 | 120*10 | 2.4 | 19/4" x 3/8" | 5.29 |
FS152A | 152*10 | 2.92 | 6" x 3/8" | 6.44 |
FS152B | 152*20 | 5.9 | 6" x 13/16" | 13 |
FS190 | 190*15 | 5.42 | 15/2" x 9/16" | 12 |
FS280 | 280*10 | 5.32 | 11" x 3/8" | 11.7 |
FS300 | 300*24 | 14.4 | 12" x 15/16" | 31.8 |
FS355 | 355*5 | 3.5 | 14" x 3/16" | 7.72 |
FS555 | 555*5 | 5.4 | 22" x 3/16" | 11.9 |
FS751 | 751*5 | 7.2 | 30" x 3/16" | 15.9 |
Markets
Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
The structural profile flat bar (isophthalic resin) is suitable for platforms, walkways, handrails, supports and various structural support locations requiring corrosion resistance and strength, and is commonly found in chemical, water treatment, power and marine engineering environments. The isophthalic resin system gives it relatively stable performance under humid and chemical media conditions. Please contact us for detailed specifications and a quotation.
Selection Guide
During selection, the required width, thickness and span of the flat bar can be checked against the dimensions and weight parameters in the table above, and the media type and load-bearing method of the service environment should be specified. If you have special requirements for cross-section, length or resin system, please contact us for detailed specifications and a quotation, and our technical staff will assist in confirming a suitable solution.
Product Advantages
This flat bar is made of glass fiber as reinforcement and resin as binder, formed by the pultrusion process. It features light weight, high strength, corrosion resistance, insulation and easy processing, and is suitable for replacing some traditional metal profiles. The isophthalic resin system helps improve durability in complex environments. Please contact us for detailed specifications and a quotation.
Inquiry Guide
For information on the size range, surface treatment, packaging method and supply arrangements of the structural profile flat bar (isophthalic resin), please contact us for detailed specifications and a quotation. Please provide the required specifications, quantity and service environment, and we will provide a corresponding solution and commercial terms accordingly.
Operating Environment
- FRP structural shapes profile is suitable for both indoor and outdoor installations, including applications exposed to weather and UV radiation.
- The glass fiber reinforced composite with resin matrix resists moisture and humid conditions, making it appropriate for coastal or high-humidity industrial settings.
- This profile performs well in corrosive environments where acids, alkalis, or salts are present, such as chemical processing plants and wastewater treatment facilities.
- It maintains stable physical properties across a wide temperature range, from cold outdoor conditions to elevated temperatures in process areas.