Product Category

Structural Profiles - Y-Profile (Vinyl Ester)


Contact us for a quotation

Product details

Greenlogy TEC

    FRP pultruded profiles are a new type of composite material that uses glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as an outer reinforcing layer. After thorough impregnation, the material is heated, formed and cured in a metal mold and then pulled by a haul-off machine in a pultrusion process. With good physical properties, these profiles are widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Y-shaped FRP profile

A*B*T


A*B*T



25*38*6.41.4

1" x 3/2" x 1/4"

3.09

38*38*6.41.6

3/2" x 3/2" x 1/4"

3.53

50*38*6.41.7

2" x 3/2" x 1/4"

3.75

Market  

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and Gsa [source term unclear — confirm]

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Entertainment and leisure

  • Telecommunications

  • Transportation

  • Water and wastewater

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal protection

  • Long service life

  • Non-conductive and thermally non-conductive

  • High strength-to-weight ratio

Raw material introduction — resin type

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type is economical with good performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

  Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles deliver years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been specified. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic modulus

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel burn test*

E-84

Flame spread

25 (max)

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volt/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies only to ISOFR and VEFR


Application Scenarios

Y-shaped FRP profiles (vinyl ester) are suitable for supporting and connecting parts that require strength, corrosion resistance and electrical insulation, such as platform edge beams, walkway handrail frames, cable tray supports and structural components in chemical environments. Specific installation locations and accessories can be confirmed against your project drawings; contact us for application advice.

Selection Guide

When selecting, first confirm the cross-section dimensions (A×B×T), single-piece length, load-bearing direction and operating environment (corrosive media, temperature, UV exposure, etc.), then determine the model against the specifications in the table above. If you provide the load conditions and installation method, we can help recommend a suitable cross-section and wall thickness.

Product Advantages

This profile uses glass fiber reinforcement and a resin matrix, formed by the pultrusion process. It offers light weight and high strength, corrosion resistance, no rusting, insulation and non-magnetic properties, and is easy to drill and cut for installation. Vinyl ester resin systems are typically used in applications with higher chemical resistance requirements; specific performance should be assessed according to operating conditions.

Inquiry Guidance

For detailed datasheets, custom lengths, surface treatment or bulk supply solutions, contact us for detailed specifications and quotations. Please provide the required cross-section, quantity, length and operating environment, and we will reply as soon as possible.

Operating Environment

  • Y-shaped FRP structural profiles are suitable for indoor and outdoor installation in industrial and civil buildings, including high-strength and long-span applications.
  • The glass fiber reinforced resin matrix resists moisture and atmospheric attack, so with correct selection the profiles are suitable for humid or coastal environments.
  • They are suitable for environments with chemical vapors, weak acids or alkalis, because the composite structure and resin binder are corrosion resistant.
  • Typical uses include structural frames, supports and profiles in factories, walkways and platforms where weather resistance and chemical resistance are required.