    FRP pultruded profiles are a new type of composite material made from glass fiber reinforcement as the raw material, resin as the binder, and glass fiber cloth as the wrapping reinforcement layer; after thorough impregnation, they are heated, formed, and cured in a metal mold and drawn out by a pulling machine. They have good physical properties and are widely used in high-strength, long-span applications.  

Type

Specification (mm)

Weight (kg/m)

Specification (in)

Weight (lbs/in)

Y-shaped Steel

A*B*T


A*B*T



25*38*6.41.4

1" x 3/2" x 1/4"

3.09

38*38*6.41.6

3/2" x 3/2" x 1/4"

3.53

50*38*6.41.7

2" x 3/2" x 1/4"

3.75

Markets  

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal resistance

  • Long service life

  • Electrical and thermal insulation

  • High strength-to-weight ratio

Introduction to raw materials — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR type with good performance and moderate acid, alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

  Greenlogy TEC pultruded fiberglass structural profiles from Greenlogy TEC are widely used in various scenarios, combining corrosion resistance, high strength, dimensional stability and light weight with thermal and electrical insulation. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile strength, LW

D-638

psi

30000

kgf/m²

21092086

Tensile strength, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive strength, LW

D-695

psi

30000

kgf/m²

21092086

Compressive strength, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural strength, LW

D-790

psi

30000

kgf/m²

21092086

Flexural strength, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Izod notched impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Izod notched impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excluding round bars and square bars

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Isophthalic Y-shaped steel is suitable for corrosive environments such as chemical processing, marine and wastewater treatment, and is also commonly used in platforms, walkways, supports and other structures requiring high strength and long spans. Its corrosion resistance, light weight and high strength give it an advantage where conventional steel is prone to rust.

Selection Guidance

When selecting, please refer to the cross-sectional dimensions (A*B*T) and weight of the Y-shaped steel for a preliminary choice based on actual load requirements, span and installation method. For precise mechanical calculations or custom sizes, please contact us for detailed specifications and a quotation.

Product Advantages

Made with isophthalic resin and glass fiber reinforcement, it offers excellent corrosion resistance and durability, while being lightweight and high in strength, making transport and installation easy. Its smooth surface and low maintenance cost suit a wide range of industrial environments.

Inquiry Guidance

For more product information, samples or bulk purchases, please contact us and we will provide professional selection advice and a quotation.

Operating Environment

  • These pultruded FRP Y-shaped steel profiles are designed for outdoor structural applications such as FRP grating walkways, platforms and handrail frames, where the glass fiber reinforcement and resin matrix resist moisture and weathering.
  • The isophthalic resin system makes the profile suitable for environments with corrosive media, including chemical plants, coastal areas and other damp industrial sites where steel sections require frequent recoating.
  • Because the profile is a non-conductive composite, it is also often chosen for structural frames near electrical equipment and other areas where steel alternatives are unsuitable.
  • For indoor installations, the same molded FRP Y-shaped steel can be used to build supports, stair treads and grating covers in wet or washdown areas; please contact us with your operating conditions to confirm the appropriate resin grade and full parameter list.