Product Category

Structural Profiles - U-Shaped Square Tube Handrail Profile (Vinyl Ester)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP pultruded profiles use glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the covering reinforcement layer. After full impregnation, they are heated, formed, and cured in a metal mold and pulled by a pulling machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

U-shaped Tube Handrail Profile

A*B*T


A*B*T



62*59*4.51.5

5/2" x 9/4" x 3/16"

3.31

62*60*51.7

5/2" x 19/8" x 3/16"

3.75

Markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Heavy-metal resistant

  • Long service life

  • Non-conductive and thermally insulating

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardancy

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type is economical with good performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Application scope:

    Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally used. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other expensive components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic modulus

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

Excluding round steel and square steel  

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardancy

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Flammability*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application scenarios

Vinyl U-shaped square-tube handrail profiles are suitable for railing and handrail systems on bridge walkways, plant platforms, and in corrosive environments such as chemical and offshore facilities, and can replace conventional metal profiles. Their surface is weather-resistant and maintenance-free, making them suitable for long-term outdoor use. Contact us with your project environment and installation method so we can recommend a suitable solution.

Selection Guide

When selecting, please consider the handrail span, load requirements and installation nodes to determine the profile cross-section dimensions and wall thickness, and check compatibility with existing railing posts and connectors. Different cross-sections and wall thicknesses correspond to different weights and mechanical performance; please refer to actual requirements for specific parameters. You are welcome to contact us for detailed specifications and quotations; our technical staff can assist in confirming the selection.

Product Advantages

This profile is pultruded from glass fiber reinforced material and resin, featuring light weight and high strength, corrosion resistance, electrical insulation and non-conductivity, and maintenance-free operation, with a long service life in humid, salt-spray and chemical media environments. The surface can be colored, and the appearance is close to metal but requires no frequent anti-corrosion treatment. You are welcome to contact us to learn about material properties and applicable working conditions.

Inquiry Guidance

For business information such as dimensions, color options, packaging methods and bulk supply, you are welcome to contact us for detailed specifications and quotations. We will provide corresponding suggestions based on your drawings or operating conditions. Please provide the required cross-section, length and quantity so that we can respond quickly.