Product Category

Structural Profiles - Three-Hole Hollow Profile (Isophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

   FRP structural profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer. After full impregnation, they are heated, formed and cured in a metal mold, and then pultruded under the pulling force of a traction machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.   

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)


450*4.5*150*618.2

18" x 3/16" x 6" x 1/4"

40.1

Market  

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Entertainment

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal resistant

  • Long service life

  • Electrically and thermally non-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardancy

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type, an economical resin with good performance and moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

   Greenlogy TEC pultruded FRP profiles are widely used in a variety of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.  

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round bars and square bars

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardancy

ASTM

Unit

Value

Tunnel test flame spread*

E-84

Flame spread

25 max

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

The three-hole hollow profile is suitable for load-bearing platforms, walkways, handrail supports, and structural components in corrosive environments such as chemical, food, and metal mining applications where strength and span requirements apply. The isophthalic resin system makes it preferable in humid and chemical-exposure conditions. For specific application suitability, please provide your operating environment parameters; you are welcome to contact us for advice.

Selection Guide

When selecting, determine the cross-section and length based on load requirements, span, support spacing, corrosive media, and installation method. The three-hole hollow structure provides a higher moment of inertia at the same weight, making it suitable for replacing some traditional profiles. Please send us your operating parameters; you are welcome to contact us for detailed specifications and selection support.

Product Advantages

Made with glass fiber reinforcement and an isophthalic resin system through the pultrusion process, it features light weight and high strength, corrosion resistance, non-conductivity, and low maintenance. The three-hole hollow cross-section helps maintain structural stiffness while reducing self-weight, and facilitates on-site cutting and installation. For specific performance data and test reports, you are welcome to contact us.

Inquiry Guidance

For information on dimensions, colors, surface treatments, and packaging and shipping options, you are welcome to contact us for detailed specifications and quotations. Please provide the required cross-section, length, quantity, and operating environment, and we will provide a corresponding solution and delivery schedule.