Product Category

Structural Profiles - Stair Tread Flat Tube (Vinyl Ester)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP pultruded profiles are made with glass fiber reinforcement, resin as the binder and glass fiber cloth as the covering reinforcement layer; after full impregnation, they are heated, formed and cured in a metal mold and pulled out by a pulling machine. This new composite material has good physical properties and is widely used in high-strength and long-span applications.  

Product type

Specification and size (mm)

Weight (kg/m)

Specification and size (in)

Weight (lbs/in)

Stair Tread Flat Tube

A*B*T1*T2


A*B*T1*T2


FT51A51*25*4*41.012" x 1" x 3/16" x 3/16"2.23
FT51B51*38*4*41.222" x 3/2" x 3/16 x 3/162.69
FT5252*32*5*51.412" x 5/4" x 3/16" x 3/16"3.11

Application markets  

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure and entertainment

  • Telecommunications

  • Transportation

  • Water and wastewater

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Safe in heavy-metal environments

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardancy

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acidic and alkaline conditions

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR resin type with good to moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

  Greenlogy TEC pultruded FRP structural profiles are widely used in various scenarios, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.  

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardancy

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies only to ISOFR and VEFR


Application Scenarios

The stair tread flat tube is used as the load-bearing frame for platform, stair and walkway treads, and is suitable for humid or corrosive environments in chemical, power, water treatment and marine applications. Its vinyl ester resin system makes it more suitable for conditions involving acid and alkali media and salt fog, and it can be combined with grating and pultruded profiles to form a complete structure.

Selection Guide

When selecting, first determine the tread length, span and load requirements, then choose the tube section size and wall thickness accordingly, and evaluate deflection based on the support spacing. Different specifications have different emphases on strength and self-weight. You are welcome to contact us for detailed specifications and a quotation, and our technical staff will help confirm a suitable model.

Product Advantages

This flat tube is pultruded from glass fiber reinforcement and vinyl ester resin, featuring light weight, high strength, corrosion resistance and electrical insulation with no magnetism. It can be cut and drilled on site for convenient installation and maintenance. Compared with traditional metal tread materials, it offers advantages in service life in corrosive environments and does not require frequent anti-corrosion coating.

Inquiry Guidance

For samples, technical documents or bulk supply plans, please provide the specification and model, quantity and operating environment, and we will reply as soon as possible. You are welcome to contact us for detailed specifications and a quotation; customized lengths and processing services are available according to project requirements.