Greenlogy TEC

  FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the adhesive, and glass fiber cloth as the covering reinforcement layer; after thorough impregnation, the material is heated, formed and cured in a metal mold, then hauled off by a pulling machine. With good physical properties, they are widely used in high-strength and long-span applications.  

Product type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Stair Tread Flat Tube

A*B*T1*T2


A*B*T1*T2


FT51A51*25*4*41.012" x 1" x 3/16" x 3/16"2.23
FT51B51*38*4*41.222" x 3/2" x 3/16 x 3/162.69
FT5252*32*5*51.412" x 5/4" x 3/16" x 3/16"3.11

Markets  

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Heavy-metal resistant

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type, economical, excellent performance, with moderate acid, alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

  Greenlogy TEC pultruded FRP structural profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in applications where steel, aluminum or wood components are traditionally specified. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.  

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic modulus

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Max %

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max 25

Flammability*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Stair tread flat tube is used for load-bearing and anti-slip support of stair steps, suitable for industrial platforms, chemical, marine and wastewater treatment and other corrosive environments. Its glass fiber reinforced composite structure remains stable under moist, salt spray and chemical medium conditions. For specific applicable environments and installation methods, please contact us for detailed specifications and quotations.

Selection Guide

When selecting, please determine the cross-section dimensions (A*B) and wall thickness (T1*T2) of the flat tube according to the stair tread span, load-bearing requirements and installation method. Different specifications correspond to different moments of inertia and load-bearing capacities; it is recommended to evaluate comprehensively in combination with tread width and support spacing. Please contact us for detailed specifications and quotations; we will assist in selection according to your working conditions.

Product Advantages

This flat tube is pultruded from glass fiber reinforced material and resin, featuring light weight, high strength, corrosion resistance, insulation and maintenance-free properties, and is suitable for replacing traditional metal tread tubes. Its surface can be processed with anti-slip treatment to improve stair safety. Please contact us for detailed specifications and quotations.

Inquiry Guide

If you need to know the specifications, performance parameters, MOQ and delivery time of stair tread flat tube, please provide cross-section dimensions, quantity and operating environment, and our technical team will reply promptly. Please contact us for detailed specifications and quotations.

Operating Environment

  • Greenlogy TEC structural profiles are composites made with glass fiber reinforcement and resin as binder, suitable for indoor and outdoor industrial installations; moisture and atmospheric exposure are normal operating conditions.
  • The glass fiber cloth covering reinforcement layer and cured resin matrix can resist corrosive media commonly found in chemical, wastewater and coastal plants, so this profile is typically used where steel requires frequent painting or replacement.
  • The stair tread flat tube in this series is used as load-bearing step support on walkways and maintenance platforms, suitable for temperature and humidity ranges common in general industrial conditions; for extreme temperatures or specific chemical exposure, please provide your project conditions and contact us.