Product Category

Structural Profiles - Square Tube (Vinyl Ester)


Contact us for a quotation

Product details

Nantong Greenlogy TEC Electronic Technology Co., Ltd.

    FRP structural profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer. After thorough impregnation, the material is heated, formed and cured in a metal mold and then pultruded under the pulling force of a haul-off machine. This new composite material has good physical properties and is widely used in high-strength, long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Square Tubing

A*B*T1*T2


A*B*T1*T2


ST25A25*25*3.2*3.20.53

1" x 1" x 1/8" x 1/8"

1.17
ST25B25*25*6.4*6.40.9

1" x 1" x 1/4" x 1/4"

1.98
ST32A32*32*3.2*3.20.7

5/4" x 5/4" x 1/8" x 1/8"

1.54
ST32B32*32*6.4*6.41.24

5/4" x 5/4" x 1/4" x 1/4"

2.73
ST38A38*38*3.2*3.20.85

3/2" x 3/2" x 1/8" x 1/8"

1.87
ST38B38*38*5*51.25

3/2" x 3/2" x 3/16" x 3/16"

2.76
ST38C38*38*6.4*6.41.54

3/2" x 3/2" x 1/4" x 1/4"

3.4
ST44A44*44*3.2*3.21.01

7/4" x 7/4" x 1/8" x 1/8"

2.23
ST44B44*44*6.4*6.41.83

7/4" x 7/4" x 1/4" x 1/4"

4.03
ST50A50*50*3.2*3.21.14

2" x 2" x 1/8" x 1/8"

2.51
ST50B50*50*3.5*3.51.24

2" x 2" x 1/8" x 1/8"

2.73
ST50C50*50*4*41.42

2" x 2" x 3/16" x 3/16"

3.13
ST50D50*50*5*51.74

2" x 2" x 3/16" x 3/16"

3.84
ST50E50*50*6.4*6.42.12

2" x 2" x 1/4" x 1/4"

4.67
ST54A54*54*3.2*3.21.24

9/4" x 9/4" x 1/8" x 1/8"

2.73
ST54B54*54*4.8*4.81.78

9/4" x 9/4" x 3/16" x 3/16"

3.92
ST60A60*60*5*52.1

19/8" x 19/8" x 3/16" x 3/16"

4.63
ST64A64*64*3.2*3.21.48

5/2" x 5/2" x 1/8" x 1/8"

3.26
ST64B64*64*4.4*4.41.97

5/2" x 5/2" x 3/16" x 3/16"

4.34
ST64C64*64*6.4*6.42.8

5/2" x 5/2" x 1/4" x 1/4"

6.17
ST76A76*76*3.2*3.21.77

3" x 3" x 1/8" x 1/8"

3.9
ST76B76*76*5*52.7

3" x 3" x 3/16" x 3/16"

5.95
ST76C76*76*6.4*6.43.39

3" x 3" x 1/4" x 1/4"

7.47
ST76D76*76*9.5*9.54.89

3" x 3" x 3/8" x 3/8"

10.8
ST89A89*89*6.4*6.43.95

7/2" x 7/2" x 1/4" x 1/4"

8.71
ST101A101*101*3.2*3.22.38

4" x 4" x 1/8" x 1/8"

5.25
ST101B101*101*5*53.61

4" x 4" x 3/16" x 3/16"

7.96
ST101C101*101*6.4*6.44.61

4" x 4" x 1/4" x 1/4"

10.2
ST152A152*152*6.4*6.47.1

6" x 6" x 1/4" x 1/4"

15.7
ST152B152*152*9.5*9.510.4

6" x 6" x 3/8" x 3/8"

22.9
ST152C152*152*12.7*12.713.5

6" x 6" x 1/2" x 1/2"

29.8
STR2525*25*3.175*3.1750.7

1" x 1" x 1/8" x 1/8"

1.54

 Markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistant

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Safe in contact with heavy metals

  • Long service life

  • Non-conductive and thermally insulating

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh acidic, alkaline and other corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical grade with excellent performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkaline environments

Applications: 

  Greenlogy TEC pultruded FRP profiles are widely used in many applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally used. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other expensive components.   

Greenlogy TEC profiles

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of linear expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Only applicable to ISOFR and VEFR


Application Scenarios

Vinyl square tubing is suitable for platforms, handrails and support structures in chemical, papermaking, electroplating and other environments with acid-base corrosion, and is also commonly used in applications requiring electromagnetic insulation and lightweight high strength. For corrosion resistance performance under specific environments, please contact us to confirm based on the medium and operating conditions.

Selection Guide

When selecting, the side length and wall thickness of the square tubing can be determined according to load, span and connection method, and general-purpose and vinyl types should be distinguished to meet different corrosion resistance requirements. If you provide the operating conditions and load conditions, we can assist in recommending suitable specifications. You are welcome to contact us for detailed specifications and quotations.

Product Advantages

This square tubing uses glass fiber as reinforcement and resin as binder, and is formed by pultrusion. It features lightweight high strength, corrosion resistance and insulation, and is suitable for replacing some metal profiles. The surface can be treated in different ways as needed; please communicate with us for specific available options.

Inquiry Guide

If you need information on the size range, weight, color and packaging of the square tubing, you are welcome to contact us for detailed specifications and quotations. Please provide the required specifications, quantity and operating environment, and we will reply as soon as possible.

Operating Environment

  • The vinyl resin square tubing in this FRP profile product line is designed for outdoor and indoor industrial environments, and is suitable for occasions where moisture, salt spray or chemical splashes would corrode steel—the pultruded glass fiber reinforcement layer bears the load, while the vinyl resin matrix provides protection.
  • Typical installation locations are walkways, platforms, handrail frames and support structures in factories, water treatment areas and coastal facilities, where square tubing can maintain dimensional stability without rusting or expanding.
  • Because this pultruded profile is formed by heat curing and pulling, its resistance to ultraviolet exposure and repeated dry-wet cycles is better than that of untreated metal, making it suitable for open-air spans exposed to sunlight, rain and washing.
  • For high-concentration acid or high-temperature conditions, please inform us of your operating conditions so that we can confirm the appropriate vinyl resin formulation and wall thickness according to your project.