Product Category

Structural Profiles - Square Tube Profiles (Isophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP profiles are a new type of composite material made with glass fiber as reinforcement, resin as adhesive, and glass fiber cloth as a covering reinforcement layer; after full impregnation, they are heated, formed, and cured in a metal mold and pultruded under the traction of a pulling machine. They have good physical properties and are widely used in high-strength, long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Square Tube Profiles

A*B*T1*T2


A*B*T1*T2


STH5050*50*6.4*53

2" x 2" x 1/4" x 3/16"

6.61

Markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and wastewater

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal resistant

  • Long service life

  • Non-conductive and thermally non-conductive

  • High strength-to-weight ratio (high specific strength)

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR type, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

    Greenlogy TEC pultruded FRP structural profiles are widely used in various scenarios, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally used. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other expensive components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic modulus

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods   

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Square tube special-shaped profiles are suitable for load-bearing and support structures with requirements on strength, span and corrosion resistance, such as building platforms, bridge and highway ancillary facilities, and chemical and food and beverage workshops. The isophthalic resin system performs well in chemical resistance and weatherability, making it suitable for long-term use in damp or corrosive environments. For specific application suitability, please consult us with your load and environmental conditions.

Selection Guide

When selecting, match the cross-section dimensions (A×B) and wall thickness (T1×T2) to the load capacity and installation interface, and refer to the dimensions and weight data in the table to estimate structural dead weight. If you need to weigh different resin systems or cross-sections, please provide your operating environment, span and load information, and we can help you determine the appropriate specification.

Product Advantages

This structural profile uses glass fiber reinforcement and resin as its matrix, formed through impregnation, molded curing and pultrusion. It offers the typical characteristics of composite materials such as light weight and high strength, corrosion resistance, electrical insulation, and ease of cutting and drilling, making it suitable for high-strength, long-span applications. Compared with traditional materials, its maintenance requirements are usually lower; specific performance depends on specification and operating conditions.

Inquiry Guidance

For detailed specifications, dimension ranges, resin system options and commercial terms for square tube special-shaped profiles, please contact us for detailed specifications and a quotation. Please provide your target cross-section, quantity and operating environment, and we will arrange technical selection and a commercial response accordingly.