Product Category

Structural Profiles - Square Tube and Special-Shaped Profiles (Vinyl Ester)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the main raw material, resin as the binder, and glass fiber cloth as the covering reinforcing layer; after full impregnation, they are heated, formed and cured in a metal mold and then pulled by a pultrusion machine. They have good physical properties and are widely used in high-strength, long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Square-Tube Profiles

A*B*T1*T2


A*B*T1*T2


STH5050*50*6.4*53

2" x 2" x 1/4" x 3/16"

6.61

Markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal safety

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin type

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinylester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR-type product with good performance and moderate acid, alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

    Greenlogy TEC pultruded FRP structural profiles are widely used in various scenarios, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles can provide many years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear strength

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods   

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face

*Applies to ISOFR and VEFR only


Application Scenarios

Vinyl ester square-tube profiles are suitable for load-bearing and structural parts requiring corrosion resistance, insulation and strength, such as building supports, cable trays and guardrails, chemical platforms, and food and beverage workshop frames. If your operating conditions involve acid-base media, outdoor aging or long-span load bearing, please contact us with details of your service environment so that we can recommend a suitable profile solution.

Selection Guide

When selecting, consider section dimensions (A×B), wall thickness (T1, T2), unit weight and installation/connection method, and determine the specification based on span, load and corrosion class. Different resin systems (such as vinyl ester) have their own emphases in corrosion resistance; please contact us to confirm specific section parameters and mechanical data.

Product Advantages

The profile uses glass fiber reinforcement and a resin matrix, formed by pultrusion, and features light weight, high strength, corrosion resistance, insulating and non-magnetic properties, and ease of cutting and installation. Glass fiber cloth serves as a wrapping reinforcement layer, enabling the product to maintain strength while adapting to long spans and harsh environments.

Inquiry Guidance

For detailed specifications, section parameters, packaging and delivery arrangements for square-tube profiles, please contact us for detailed specifications and a quotation. Please provide the required section dimensions, quantity and service environment, and we will match a suitable product solution accordingly.