  Pultruded FRP profiles are a new type of composite material made with glass fiber reinforcement as the base material and resin as the matrix, with glass fiber cloth as the outer reinforcing layer; after thorough impregnation, they are heated, formed and cured in a metal mold and then pulled and drawn by a pulling machine. They have good physical properties and are widely used in high-strength, long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Solid Square Rod

A*B
A*B
SSR2525*251.231" x 1"2.71
SSR3232*3225/4" x 5/4"4.41
SSR3838*382.83/2" x 3/2"6.17

Markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Can be safely used in heavy metal environments

  • Long service life

  • Electrically and thermally non-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR-type resin with good, moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

    Greenlogy TEC pultruded FRP structural profiles are widely used in a variety of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally selected. Today these profiles are often used in highly corrosive applications that previously required stainless steel and other expensive components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Izod notched impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Izod notched impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Structural Profiles - Solid Square Rod (Vinylester), with its composite structure of glass fiber reinforcement and resin matrix, is suitable for load-bearing and support applications requiring high strength and larger spans, such as building structures, bridge auxiliary components, industrial platform handrails, and frame connections in corrosive environments. For suitability in specific projects, please contact us to discuss your operating conditions.

Selection Guidance

During selection, you may refer to the cross-sectional dimensions and unit weight of existing specifications (SSR25, SSR32, SSR38, etc.) for preliminary matching based on load requirements, installation space, and corrosion resistance needs. If you have questions about load capacity, span, or connection methods, please contact us for detailed specifications and a quotation, and our technical staff will assist with confirmation.

Product Advantages

This product uses glass fiber cloth as the reinforcement layer; it is impregnated with resin, heat-cured in a metal mold, and pultruded, offering good physical properties and structural stability suitable for high-strength, large-span use. The vinylester material also helps improve corrosion resistance. Please contact us for detailed specifications and a quotation.

Inquiry Guidance

If you wish to purchase Structural Profiles - Solid Square Rod (Vinylester), please provide the required specifications, quantity, and operating environment, and we will propose a suitable solution accordingly. Please contact us for detailed specifications and a quotation, and we will respond to your inquiry as soon as possible.

Operating Environment

  • These pultruded solid square rods are designed for structural frames that are both exposed to indoor plant atmospheres and outdoors, and their glass fiber reinforcement and resin matrix resist moisture and weathering, whereas untreated steel would corrode under these conditions.
  • Suitable for humid and chemically corrosive environments, such as wastewater treatment, chemical processing, and coastal locations, where composite profiles do not rust and maintain their shape without painting.
  • Typical uses include walkway supports, handrail posts, platform frames, and grating clamping components, suitable for indoor and outdoor use and able to withstand temperature fluctuations in normal industrial service.
  • For long-term exposure to concentrated acids, strong alkalis, or continuous high temperatures, please inform us of the medium and temperature so that the resin system can be matched to your site conditions before ordering.