Product Category

Structural Profiles - Solid Square Rod (Orthophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP structural profiles are made of glass fiber reinforced material, with resin as the binder and glass fiber cloth as the covering reinforcement layer. After thorough impregnation, they are heated, formed and cured in a metal mold, and then pulled by a haul-off machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Solid Square Rod

A*B
A*B
SSR2525*251.231" x 1"2.71
SSR3232*3225/4" x 5/4"4.41
SSR3838*382.83/2" x 3/2"6.17

Markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Safe in heavy-metal environments

  • Long service life

  • Electrical and thermal insulation (non-conductive, non-heat-conductive)

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical, with excellent performance and resistance to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

    Greenlogy TEC pultruded FRP structural profiles from Greenlogy TEC are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal and electrical insulation. Durable Greenlogy TEC profiles deliver years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max 25

Flame resistance*

D-635

---

Non-burning

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Solid square rods are suitable for high-strength, long-span structural supports, connectors and various load-bearing frames, and perform particularly well in construction, bridges and industrial platforms where corrosion resistance and light weight are required. Their smooth surface and stable cross-section also facilitate secondary processing and installation.

Selection Guide

When selecting, please determine the side length and length of the square rod based on structural loads, spans and environmental conditions, and also consider the installation method and connection requirements. We offer a variety of size specifications; please contact us for detailed specifications and selection support.

Product Advantages

Made with orthophthalic (phthalic acid-type) resin and glass fiber reinforcement, solid square rods offer excellent mechanical properties, corrosion resistance and electrical insulation, and are lightweight and easy to cut and drill. Their surface is flat and their dimensions are stable, making them suitable for engineering applications with high strength and durability requirements.

Inquiry Guidance

For specific specifications, prices or customization needs, please contact us for detailed specifications and a quotation. Our technical team will provide professional advice based on your project.

Operating Environment

  • These pultruded solid square rods are suitable for indoor and outdoor installation; their glass fiber reinforcement and cured resin matrix resist moisture, humidity and weathering better than untreated steel.
  • Typical operating conditions include exposure to mild acids, alkalis, salts and other corrosive media found in chemical workshops, water treatment areas and coastal sites; the vinyl ester resin system (phthalic acid type) gives the profiles their corrosion resistance in these harsh environments.
  • Because the material is non-conductive and non-magnetic, the square rods are also used in environments requiring electrical insulation or electromagnetic wave transparency, such as near live equipment or in instrument supports.
  • Long-term outdoor exposure to UV and temperature cycling does not cause rust or galvanic corrosion as metal profiles do, making these structural profiles a practical choice for year-round use in bridge, walkway and platform applications.