Structural Profiles - Solid Square Rod (Isophthalic)
Product details
Greenlogy TEC
FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the adhesive, and glass fiber cloth as the covering reinforcement layer; after full impregnation with resin, the material is heated, molded and cured in a metal die and then pulled by a haul-off machine. With good physical properties, they are widely used in high-strength and long-span applications.
Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Solid Square Rod | A*B | A*B | ||
| SSR25 | 25*25 | 1.23 | 1" x 1" | 2.71 |
| SSR32 | 32*32 | 2 | 5/4" x 5/4" | 4.41 |
| SSR38 | 38*38 | 2.8 | 3/2" x 3/2" | 6.17 |
Markets
Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Leisure
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistance
Low maintenance
Flame retardant
Low installation cost
Safe in heavy-metal environments
Long service life
Non-conductive, non-thermal-conductive
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type: economical, excellent performance, resistant to moderate acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with non-conductive and non-thermal-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas traditionally built with steel, aluminum or wood components. Today, these profiles are often used in highly corrosive applications where stainless steel and other costly components were previously required.
Greenlogy TEC profiles
Mechanical properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of elasticity | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-beam shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod impact strength, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod impact strength, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | Max. % | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max. 25 |
Combustibility* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face
*Applies to ISOFR and VEFR only
Application Scenarios
Solid square rods are suitable for load-bearing, support and connection structures that require strength and durability, such as building frames, bridge ancillary components, platform handrails and industrial equipment supports. Their lightweight, high-strength and corrosion-resistant properties also suit corrosive environments such as chemical and marine applications. Specific applicable scenarios can be confirmed according to project requirements.
Selection Guide
When selecting, determine the side length and length of the square rod based on load, span and service environment (corrosion, temperature, etc.), and refer to the dimensions and weights in the table for preliminary matching. If combination with other profiles or secondary processing is required, please specify the connection method and processing requirements. You are welcome to contact us for detailed specifications and selection advice.
Product Advantages
This solid square rod is made of isophthalic resin and glass fiber reinforcement, offering high specific strength, good corrosion resistance and electrical insulation, and is non-magnetic and easy to machine. Compared with traditional metal materials, it is lighter, easier to transport and install, and suitable for applications requiring high durability.
Inquiry Guide
For more specifications, technical parameters or a quotation, please contact us. Please provide the required dimensions, quantity and service environment, and we will provide a detailed solution and commercial support as soon as possible.
Service Environment
- These solid square rods are pultruded from glass fiber reinforcement and an isophthalic resin matrix, giving the profiles moisture resistance and resistance to a range of industrial chemicals in indoor and outdoor use.
- Typical applications are structural frames that would corrode steel under damp, salt-fog or washdown conditions, such as weather-exposed platforms, walkways and support frames.
- The isophthalic resin system is suitable for environments with moderate chemical exposure, including industrial plants and water treatment areas where condensation and splash contact occur.
- For continuous use, keep the profiles within the temperature and chemical limits of the resin system; for guidance on the environment and parameters of a specific project, please contact Greenlogy TEC.