Structural Profiles - Solid Round Rod (Vinyl Ester)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP pultruded profiles are made with glass fiber as the reinforcement, resin as the binder, and glass fiber cloth as the outer reinforcing layer; after full impregnation, they are heated, formed and cured in a metal die and then pulled by a pulling machine. This new composite material has good physical properties and is widely used in high-strength, long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Solid Round Rod

D
D
SRR6060.081/4"0.18
SRR959.50.143/8"0.31
SRR12712.70.261/2"0.57
SRR25425.411"2.2
SRR32831.81.515/4"3.33
SRR380382.153/2"4.74
SRR424.20.033/16"0.07
SRR808.00.15/16"0.22
SRR16160.415/8"0.9
SRR19190.553/4"1.21
SRR20200.6213/16"1.37
SRR22220.727/8"1.59

Markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Heavy metal resistance

  • Long service life

  • Electrically and thermally insulating

  • High specific strength

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical, good performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

    Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications that would otherwise require stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame retardancy*

D-635

---

Non-burning

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Vinyl solid round rods are suitable for load-bearing and insulating components requiring strength, insulation and corrosion resistance, such as chemical platform supports, electrical insulating rods, and marine and wastewater treatment structural parts. They are also commonly used for custom machined parts and sports equipment rods. Contact us to confirm a suitable solution based on your operating conditions.

Selection Guide

When selecting vinyl solid round rods, please confirm the required diameter, length, load-bearing method, operating environment (media, temperature, outdoor exposure) and surface requirements. For insulation or long-term corrosive environments, we recommend providing detailed operating conditions so we can help determine the appropriate resin system and fiber arrangement. Contact us for detailed specifications and selection advice.

Product Advantages

This solid round rod is made of glass fiber reinforcement with a vinyl resin matrix and produced by pultrusion. It features light weight, high strength, insulation, corrosion resistance and weather resistance. It has a smooth surface and can be cut and machined as needed, making it suitable for high-strength, long-span structural requirements. Specific performance varies by specification and process; contact us for the corresponding data.

Inquiry Guidance

For information on the size range, performance parameters, customization possibilities and commercial terms of vinyl solid round rods, please contact us. Provide the required diameter, length, quantity and operating environment, and we will reply as soon as possible. Contact us for detailed specifications and a quotation.

Operating Environment

  • Vinyl-type solid round rods are used for indoor and outdoor structural components, including walkways, platforms and support frames, where long-term exposure to weathering and humid environments is expected.
  • The vinyl resin matrix and glass fiber reinforcement enable the rods to resist corrosive media commonly found in chemical plants, wastewater treatment and coastal facilities, including splash and vapor exposure.
  • These rods are suitable for humid or condensation-prone areas and will not corrode like steel when exposed to water or salt-laden air.
  • For high-temperature conditions, chemical compatibility or load requirements beyond the standard range of use, please contact Greenlogy TEC and provide your project conditions so we can confirm suitable specifications.