Structural Profiles - Solid Round Rod (Isophthalic)
Product details
Nantong Greenlogy TEC Electronic Technology Co., Ltd.
FRP pultruded profiles are made from glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the surfacing reinforcement layer. After thorough impregnation, they are heated, formed and cured in a metal mold and pulled by a haul-off machine to produce a new type of composite material with good physical properties, widely used in high-strength, long-span applications.
Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Solid Round Rod | D | D | ||
| SRR60 | 6 | 0.08 | 1/4" | 0.18 |
| SRR95 | 9.5 | 0.14 | 3/8" | 0.31 |
| SRR127 | 12.7 | 0.26 | 1/2" | 0.57 |
| SRR254 | 25.4 | 1 | 1" | 2.2 |
| SRR328 | 31.8 | 1.51 | 5/4" | 3.33 |
| SRR380 | 38 | 2.15 | 3/2" | 4.74 |
| SRR42 | 4.2 | 0.03 | 3/16" | 0.07 |
| SRR80 | 8.0 | 0.1 | 5/16" | 0.22 |
| SRR16 | 16 | 0.41 | 5/8" | 0.9 |
| SRR19 | 19 | 0.55 | 3/4" | 1.21 |
| SRR20 | 20 | 0.62 | 13/16" | 1.37 |
| SRR22 | 22 | 0.72 | 7/8" | 1.59 |
Markets
Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Recreation
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistant
Low maintenance
Flame retardant
Low installation cost
Heavy metal resistant
Long service life
Electrically and thermally non-conductive
High specific strength
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type: economical, good performance, resistant to moderate acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded fiberglass structural profiles are widely used in various scenarios, combining corrosion resistance, high strength, dimensional stability and light weight, with low thermal conductivity and electrical insulation. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Mechanical properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, longitudinal | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, transverse | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, longitudinal | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, transverse | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, longitudinal | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, transverse | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, longitudinal | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, transverse | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, longitudinal | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, transverse | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, longitudinal | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, transverse | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of elasticity | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-beam shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod impact strength, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod impact strength, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical Properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | 25 max |
Flame resistance* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face
*Only applicable to ISOFR and VEFR
Application Scenarios
Isophthalic solid round rods are commonly used for support, connection and load-bearing components that require both strength and corrosion resistance, such as platform handrail posts, grating support rods, equipment tie rods and various structural reinforcements. In high-humidity, acid-base or salt-spray environments, the isophthalic resin system can provide more stable long-term performance, making it suitable for working conditions in chemical, water treatment, marine and power industries. For specific application recommendations, please contact us to confirm based on your working conditions.
Selection Guide
When selecting, focus mainly on the required diameter, load form (tension/compression/bending), support span and the corrosion level of the service environment, and use these to determine the required cross-sectional size and resin system. Isophthalic solid round rods are more suitable for occasions with stronger corrosiveness or higher durability requirements; for general indoor structures, cost can be evaluated comprehensively. You are welcome to contact us with your working condition parameters so we can help match the appropriate specifications.
Product Advantages
This product uses glass fiber as reinforcement and resin as matrix, and is formed by impregnation, heating curing and pultrusion. It features light weight, high strength, corrosion resistance, electrical insulation and non-magnetic properties, and is easy to cut and machine. The solid round rod has a dense cross-section, stable compressive and flexural performance, and is convenient for drilling, turning and combined installation with other structural parts. Compared with traditional metal materials, it can reduce maintenance requirements in corrosive environments.
Inquiry Guidance
If you would like to know the detailed specifications, size range, resin system options and supply information of this series of solid round rods, please contact us. We will provide selection recommendations and quotation proposals according to your working conditions. You may also provide the required diameter, length, quantity and service environment so that we can reply faster.
Service Environment
- This solid round rod is produced with isophthalic resin, offering enhanced water resistance and broad resistance to corrosive media, and is suitable for indoor and outdoor installation.
- Typical service environments for this FRP structural profile include humid and chemical exposure areas, such as industrial plants, wastewater treatment facilities, and marine or coastal areas where steel would corrode.
- The pultruded glass fiber reinforced structure allows this round rod to be used over a wide temperature range without losing structural integrity; please contact us for detailed temperature performance data.
- Because the material is non-conductive and corrosion resistant, it is often used in applications near acids, alkalis, salts and other aggressive media; specific chemical compatibility should be confirmed with our technical team.