   FRP pultruded profiles are a new composite material made with glass fiber reinforcement as the base, resin as the binder, and glass fiber cloth as the covering reinforcement layer; after full impregnation, the material is heated, formed and cured in a metal mold and then pultruded by a pulling machine. With good physical properties, they are widely used in high-strength, long-span applications.   

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)


1000*140*531.6

39" x 11/2" x 3/16"

69.7

Markets 

  • Construction

  • Bridges and Highways

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metals and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Recreation

  • Communications

  • Transportation

  • Water and Wastewater

Features:

  • Corrosion resistance

  • Low maintenance requirements

  • Flame retardant

  • Low installation cost

  • Heavy metal resistant

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Introduction to raw materials — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinylester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR-type resin with good moderate acid, alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:  

   Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal insulation and non-conductivity. Durable Greenlogy TEC profiles offer years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.  

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic modulus

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round bars and square bars

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

The seven-hole partition panel is suitable for locations requiring clean, corrosion-resistant and lightweight partitioning, such as plant and laboratory partitions in the chemical, food and beverage, electronics manufacturing and other industries. Its FRP material is easy to wash and clean, and it is also commonly used in internal partition walls of bridge and tunnel ancillary facilities and municipal engineering. For specific scenario suitability recommendations, please contact us.

Selection Guidance

When selecting, it is recommended to first confirm the partition's load conditions, span, service environment (humidity, chemical exposure) and installation method, then evaluate based on panel section dimensions and unit weight. If coordination with existing structures, suspended ceilings, or door and window openings is required, please provide drawings or dimensional requirements, and we can assist in matching specifications. For detailed selection parameters, please contact us.

Product Advantages

This partition panel is made of glass fiber reinforced material composited with resin, formed by molding and pultrusion. It features high strength, light weight, corrosion resistance, insulation and maintenance-free performance, making it suitable for large spans and humid environments. The surface is flat and can be cut and drilled, facilitating on-site installation. For certifications and performance data, please contact us.

Inquiry Guidance

To learn about the specifications, colors, surface treatments and supply methods of the seven-hole partition panel, please contact us for detailed specifications and quotations. Please inform us of the service environment, required dimensions and quantity, and we will provide selection recommendations and commercial terms accordingly.

Service Environment

  • The seven-hole FRP partition panel is made of glass fiber reinforced material with resin as the binder and is equipped with a glass fiber cloth covering reinforcement layer, so it is suitable for both indoor installation and outdoor structures subject to humidity and weather exposure.
  • Because the resin matrix and glass fiber reinforcement can resist chemical attack, this pultruded partition panel is often used in chemical, food and beverage, metal and mining, and microelectronics facilities where corrosive media and washdown conditions exist.
  • This panel is suitable for buildings, bridges and highways, and manufacturing environments, where humidity fluctuations and sustained service loads are normal operating conditions.
  • To learn about temperature limits, chemical resistance ratings and the complete parameter list, please contact us with your project conditions.