   FRP profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the covering reinforcement layer. After thorough impregnation, they are heated, formed and cured in metal molds, then pultruded by a pulling machine. This new composite material offers good physical properties and is widely used in high-strength, long-span applications.   

Grade

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)


1000*140*531.6

39" x 11/2" x 3/16"

69.7

Markets 

  • Construction

  • Bridges and Highways

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metals and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and Wastewater Treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Safe in heavy-metal environments

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Severe acid, alkali and other corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR type with good, moderate acid, alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:  

   Greenlogy TEC pultruded FRP structural profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with non-thermal-conductive and non-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.  

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Izod notched impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Izod notched impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies only to ISOFR and VEFR


Application Scenarios

The seven-hole partition wall board (isophthalic) is suitable for partition walls, platforms, walkways and equipment enclosures that require both corrosion resistance and structural strength, and is commonly found in corrosive environments such as chemical, food, electroplating and water treatment facilities. The isophthalic resin system performs stably in resistance to chemical media and damp heat, making it suitable for areas exposed long-term to humid or mildly acidic/alkaline atmospheres. For specific application suitability, please contact us to confirm based on your site conditions.

Selection Guidance

When selecting, take into account the medium type and concentration in the service environment, long-term working temperature, span and load conditions, and the installation and fixing method. The seven-hole structure reduces self-weight while maintaining the section moment of inertia, making it suitable for partition applications that are weight-sensitive or require large spans. As this catalog entry does not list complete mechanical and corrosion-resistance data, please contact us for detailed specifications and selection support.

Product Advantages

This profile uses fiberglass reinforcement with an isophthalic resin matrix, formed by the pultrusion process, and offers the typical composite characteristics of light weight, high strength, corrosion resistance, non-conductivity and low maintenance. The seven-hole cross-section increases stiffness for the same material usage, is easy to cut and install on site, and can reduce the frequency of later maintenance and replacement. Actual performance is subject to testing and the technical agreement of the order.

Inquiry Guidance

For information on dimensional tolerances, color, surface treatment, packaging and bulk supply solutions, please contact us for detailed specifications and a quotation. Please provide details such as the service environment, span, load and quantity, and we will recommend suitable specifications and arrange technical follow-up accordingly.

Service Environment

  • A structural profile made from glass fiber reinforcement bonded with pultruded resin, suitable for normal use in indoor factories, outdoor structures and semi-enclosed industrial areas where temperature and humidity fluctuate with the seasons.
  • The molded cured surface of these FRP structural profiles resists moisture and the corrosive splashes, vapors and chemically laden air found in chemical, food and beverage, metal and mining processing environments, so the profiles require no paint protection.
  • Because the glass fiber cloth reinforcement layers are fully impregnated with resin, the profiles retain their shape and load-bearing function in high-strength, long-span installations such as partition frames and support structures exposed to washdown or humid process areas.
  • For use in a specific medium or at a specified temperature or humidity level, please provide your project conditions and contact us so that the profile selection can be confirmed against the full parameter table; no universal usage limitation applies.