Product Category

Structural Profiles - Seven-Hole Hollow Profile (Vinyl Ester)


Contact us for a quotation

Product details

Greenlogy TEC

   Pultruded FRP profiles are a new type of composite material made with glass fiber reinforcement as the main material, resin as the adhesive, and glass fiber cloth as the covering reinforcement layer; after thorough impregnation, they are heated, formed, and cured in a metal mold and pulled by a pulling machine. They offer excellent physical properties and are widely used in high-strength, long-span applications.   

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)


600*8.5*56*825.4

24" x 5/16" x 2" x 5/16"

56

Application markets 

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Safe in heavy-metal environments

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin type

Code

Resin type

Flame retardant performance

Standard color

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Grass green, yellow, gray, orange

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

An economical VEFR product with good performance and moderate acid, alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

General acid and alkali environments

Applications:  

   Greenlogy TEC pultruded FRP profiles are widely used by Greenlogy TEC in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally used. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other expensive components.  

Greenlogy TEC Profiles

Mechanical Properties

ASTM

Unit

值(v)

Unit

值(v)

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact, Longitudinal

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact, Transverse

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square bars

Physical Properties

ASTM

Unit

值(v)

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Max %

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, longitudinal

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

值(v)

Tunnel test*

E-84

Flame spread

Max. 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

值(v)

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = longitudinal, CW = crosswise, PF = perpendicular to laminate face

*Applies only to ISOFR and VEFR


Applications

The seven-hole hollow profile (vinyl ester) is suitable for applications requiring strength, corrosion resistance and light weight, such as building platforms, bridge walkways, chemical operating platforms, food processing equipment supports, manufacturing production lines and metal mining. Its structural design facilitates load-bearing and spanning applications and meets the requirements of various industrial environments.

Selection Guidance

When selecting, factors such as load requirements, span, support conditions and environmental corrosiveness should be considered comprehensively. The seven-hole hollow profile is available in different sizes and specifications, allowing the appropriate cross-section to be selected according to actual structural requirements. Contact us for detailed specifications and selection advice; our technical team will assist you with the selection.

Product Advantages

This profile is made from glass fiber reinforced material compounded with resin and formed by the pultrusion process. It features light weight, high strength, corrosion resistance and fatigue resistance. The seven-hole hollow structure reduces self-weight while maintaining mechanical performance, making installation and transport easier and making it suitable for long-span structures.

Inquiry Guidance

For detailed specifications, technical parameters or commercial terms for the seven-hole hollow profile (vinyl ester), please contact us for specifications and a quotation. We can provide customized solutions according to your project requirements.

Operating Environment

  • This vinyl ester structural profile is pultruded from glass fiber reinforced material, resin and glass fiber cloth, and is suitable for indoor factory installation and outdoor structural applications.
  • Its pultruded FRP structure makes it suitable for use in humid and chemically corrosive environments, such as chemical, food and beverage, and metal and mining facilities.
  • With its high strength-to-weight ratio, the seven-hole hollow profile is used in construction, bridges and highways, and manufacturing projects where long spans are required.
  • For exact temperature resistance and exposure limits, please contact us for a complete parameter list before specifying this profile.