Structural Profiles - Round Tube (Isophthalic)
Product details
Greenlogy TEC
FRP profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the covering reinforcement layer; after thorough impregnation, they are heated, formed and cured in a metal mold and pultruded under the traction of a pulling machine. With good physical properties, they are widely used in high-strength and long-span applications.
Type | Specification (mm) | Weight (kg/m) | Specification (in) | Weight (lbs/in) |
|---|---|---|---|---|
Round Tube | D*T | D*T | ||
| RT25 | 25*3.2 | 0.44 | 1" x 1/8" | 0.97 |
| RT26A | 26*3 | 0.42 | 1" x 1/8" | 0.93 |
| RT26B | 26*4.8 | 0.63 | 1" x 3/16" | 1.39 |
| RT32A | 32*3.2 | 0.55 | 5/4" x 1/8" | 1.21 |
| RT32B | 32*5 | 0.81 | 5/4" x 3/16" | 1.79 |
| RT32C | 32*6 | 0.96 | 5/4" x 1/4" | 2.12 |
| RT38A | 38*3.2 | 0.65 | 3/2" x 1/8" | 1.43 |
| RT38B | 38*4 | 0.81 |
3/2" x 3/16"
| 1.79 |
| RT38C | 38*5 | 1 | 3/2" x 3/16" | 2.2 |
| RT38D | 38*6.4 | 1.18 | 3/2" x 1/4" | 2.6 |
| RT41 | 41*4.5 | 0.98 | 13/8" x 3/16"
| 2.16 |
| RT42A | 42*3.2 | 0.7 | 13/8" x 1/8" | 1.54 |
| RT42B | 42*5 | 1.11 | 13/8" x 3/16" | 2.45 |
| RT42C | 42*6.4 | 1.45 | 13/8" x 1/4" | 3.2 |
| RT48 | 48*6.4 | 1.58 | 15/8" x 1/4" | 3.48 |
| RT50A | 50*3.2 | 0.84 | 2" x 1/8" | 1.85 |
| RT50B | 50*4 | 1.1 | 2" x 3/16" | 2.43 |
| RT50C | 50*5 | 1.34 | 2" x 3/16" | 2.95 |
| RT50D | 50*6.4 | 1.67 | 2" x 1/4" | 3.68 |
| RT50E | 50*3.5 | 0.96 | 2" x 1/8" | 2.12 |
| RT50.8A | 50.8*6.4 | 1.7 | 2" x 1/4" | 3.75 |
| RT50.8B | 50.8*3.2 | 0.86 | 2" x 1/8" | 1.9 |
| RT64A | 64*3.5 | 1.26 | 5/2" x 1/8" | 2.78 |
| RT64B | 64*6.4 | 2.38 | 5/2" x 1/4" | 5.25 |
| RT75 | 75*4.2 | 1.8 | 3" x 3/16" | 3.97 |
| RT76 | 76*6.4 | 2.64 | 3" x 1/4" | 5.82 |
| RT89A | 89*3.2 | 1.54 | 7/2" x 1/8"
| 3.4 |
| RT89B | 89*5 | 2.51 | 7/2" x 3/16"
| 5.35 |
| RT89C | 89*6.4 | 3.13 | 7/2" x 1/4" | 6.9 |
| RT99 | 99*5 | 2.81 | 4" x 3/16" | 6.19 |
| RT101 | 101*6.4 | 3.62 | 4" x 1/4" | 7.98 |
| RT114A | 114*3.2 | 2.12 | 9/2" x 1/8" | 4.67 |
| RT114B | 114*5 | 3.25 | 9/2" x 3/16"
| 7.17 |
| RT114C | 114*6.4 | 4.11 | 9/2" x 1/4" | 9.06 |
| RT114D | 114*9.5 | 5.93 | 9/2" x 3/8" | 13.07 |
| RT150A | 150*3.2 | 2.81 | 6" x 1/8" | 6.19 |
| RT150B | 150*5 | 4.35 | 6" x 3/16" | 9.59 |
| RT150C | 150*6.4 | 5.5 | 6" x 1/4"
| 12.1 |
| RT150D | 150*9.5 | 8 | 6" x 3/8" | 17.6 |
Application markets
Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Recreation
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistance
Low maintenance
Flame retardant
Low installation cost
Resistance to heavy metals
Long service life
Electrically and thermally insulating
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Harsh corrosive environments such as acids, alkalis and other corrosive media |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type: economical, good performance, resistant to moderate acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in applications where steel, aluminum or wood components are traditionally used. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of linear expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | 25 max |
Flame resistance* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | V/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face
*Applies only to ISOFR and VEFR
Application Scenarios
Round tube profiles are commonly used in load-bearing and support structures where strength and span are required, such as platform handrails, ladders, grating support beams, cable tray brackets, and frame components in corrosive environments such as chemical plants and coastal areas. The isophthalic resin system is suitable for working conditions with higher corrosion resistance requirements; please contact us to discuss specific application scenarios.
Selection Guide
When selecting, first confirm whether the outer diameter and wall thickness (D*T) meet the fitting and load-bearing requirements of the connectors, then evaluate the cross-section size based on span, support method, and operating environment; the table provides both metric and imperial specifications for easy correspondence with existing design drawings. If you need to balance strength, stiffness, and weight, please provide your working conditions and we will assist with selection.
Product Advantages
Pultruded round tubes use glass fiber as reinforcement and resin as matrix, and are continuously formed through impregnation, heating, and curing. They feature light weight and high strength, corrosion resistance, non-magnetic properties, electrical insulation, and ease of cutting and drilling, making them suitable for replacing some metal pipes in corrosive or insulating applications. The isophthalic resin formulation offers more stable performance in water and chemical media resistance.
Inquiry Guide
For detailed specifications, available size ranges, surface treatment options, and packaging and shipping arrangements for round tubes, please contact us for detailed specifications and a quotation. Please provide the required outer diameter, wall thickness, length, quantity, and operating environment, and we will respond with a corresponding solution.