Structural Profiles - Kick Plate (Vinyl Ester)
Product details
Greenlogy TEC
FRP pultruded profiles are made from glass fiber reinforced material as the raw material, resin as the binder, and glass fiber cloth as the wrapping reinforcing layer; after full impregnation, they are heated, formed, and cured in a metal mold and pulled by a haul-off machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.
Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Kick Plate | A*B*T | A*B*T | ||
M2 | 100*13*3.2 M型 | 1.1 | 4" x 1/2" x 1/8" M型
| 2.43 |
M3 | 100*16*5 M型 | 1.3 | 4" x 5/8" x 3/16" M型 | 2.87 |
M4 | 148*12*3 M型 | 1.27 | 23/4" x 1/2" x 1/8" M型 | 2.8 |
W1 | 100*19*5 W型 | 1.36 | 4" x 3/4" x 3/16" W型 | 3 |
W2 | 100*15*3.2 W型 | 1.1 | 4" x 9/16" x 1/8" W型 | 2.43 |
W3 | 150*15*3.2 W型 | 1.6 | 6" x 9/16" x 1/8" W型 | 3.53 |
Markets
Construction
Bridges and Highways
Chemical
Food and Beverage
Manufacturing
Metals and Mining
Microelectronics
Oil and Gas
Pharmaceutical
Power
Pulp and Paper
Recreation
Telecommunications
Transportation
Water and Wastewater Treatment
Features:
Corrosion resistance
Low maintenance
Flame retardant
Low installation cost
Heavy metal resistance
Long service life
Electrical and thermal insulation
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Suitable for harsh corrosive environments such as acids and alkalis |
IFR-25 | Isophthalic type | Oxygen index 28 and above | The VEFR type is an economical product with good performance and moderate acid, alkali and solvent resistance |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP profiles are widely used, combining corrosion resistance, high strength, dimensional stability and light weight with thermal and electrical insulation properties. Where steel, aluminum or wood members have traditionally been specified, durable Greenlogy TEC profiles offer years of low-maintenance service. Today these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Mechanical properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Elastic modulus | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-beam shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod impact, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod impact, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | Maximum percentage | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Maximum 25 |
Combustibility* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface
*Applies to ISOFR and VEFR only
Application Scenarios
Vinyl kick plate structural profiles are commonly used for edge protection of platforms, walkways and equipment in corrosive environments such as chemical processing, electroplating and water treatment, and can be installed together with FRP grating and pultruded profiles. If you need to confirm suitability for a specific operating condition, please contact us to discuss.
Selection Guide
When selecting, consider the dimensions of the mounting surface, the required cross-sectional shape (such as M-shape), and the load-bearing and protection requirements, then choose a similar specification from the existing size chart. For non-standard sizes or special cross-section requirements, please contact us for detailed specifications and a quotation.
Product Advantages
This profile is pultruded from glass fiber reinforcement and resin, offering corrosion resistance, high strength and light weight, making it suitable for replacing some metal kick plates in damp or chemically exposed environments. Specific performance can be further discussed based on project requirements.
Inquiry Guide
To learn about detailed specifications, supply forms and commercial terms for vinyl kick plate structural profiles, please contact us for detailed specifications and a quotation. We can provide selection advice and technical support based on your application needs.
Operating Environment
- This vinyl kick plate from the FRP pultruded profile product line is suitable for indoor and outdoor installation, resists moisture and will not expand or warp.
- The vinyl surface provides lasting protection against routine chemical splashes and corrosive media common in industrial environments, extending service life in demanding plant conditions.
- The kick plate maintains performance across the wide temperature range common in industrial and commercial applications, retaining its shape and structural integrity under high-temperature, low-temperature and humid conditions.
- The profile uses a pultruded FRP core, withstanding long-term outdoor weather exposure and washdown operations, making it a practical choice for platforms, walkways and process areas.