Product Category

Structural Profiles - Kick Plate (Isophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP pultruded structural profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer; after full impregnation, they are heated, formed and cured in a metal mold and pulled by a pulling machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Toe Board

A*B*T


A*B*T


M2

100*13*3.2 M型

1.1

4" x 1/2" x 1/8" M型

2.43

M3

100*16*5 M型

1.3

4" x 5/8" x 3/16" M型

2.87

M4

148*12*3 M型

1.27

23/4" x 1/2" x 1/8" M型

2.8

W1

100*19*5 W型

1.36

4" x 3/4" x 3/16" W型

3

W2

100*15*3.2 W型

1.1

4" x 9/16" x 1/8" W型

2.43

W3

150*15*3.2 W型

1.6

6" x 9/16" x 1/8" W型

3.53

Market 

  • Construction

  • Bridge and highway

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metal and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation and entertainment

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Resistant to heavy metal hazards

  • Long service life

  • Electrical and thermal insulation

  • High specific strength

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR-type product with good performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

 Applications: 

   Greenlogy TEC pultruded FRP profiles from Greenlogy TEC are used across a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductive properties. In areas where steel, aluminum or wood components have traditionally been specified, durable Greenlogy TEC profiles provide years of low-maintenance service. Today these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile Stress, Lengthwise

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, Crosswise

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, Lengthwise

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, Crosswise

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, Lengthwise

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, Crosswise

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, Lengthwise

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, Crosswise

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, Lengthwise

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, Crosswise

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, Lengthwise

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, Crosswise

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact, Lengthwise

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact, Crosswise

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical Properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flammability*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

This isophthalic structural profile toe board is suitable for platform, walkway, tank farm and trench edge protection where corrosion resistance and load-bearing are required, providing protection, edge sealing and a finished appearance. It is commonly used with FRP grating or profiles in chemical, wastewater treatment, electroplating, marine engineering and similar environments. For specific environmental suitability, please contact us for detailed specifications and a quotation.

Selection Guide

During selection, the cross-section dimensions A*B*T and models such as M2, M3 and M4 can be determined based on the span, load and fixing method at the installation location. The isophthalic resin system is suitable for highly corrosive working conditions. If it is to be used with other FRP profiles or grating, we recommend providing drawings or on-site dimensions. For detailed specifications and a quotation, please contact us.

Product Advantages

Using glass fiber reinforcement and isophthalic resin as the matrix, it is formed through heating, molding, curing and pultrusion, offering good mechanical properties, corrosion resistance and dimensional stability, and is suitable for high-strength, long-span applications. Different surface treatments can be selected according to requirements, making installation and maintenance easier. Please contact us for detailed specifications and a quotation.

Inquiry Guide

To confirm the dimensions, color, length and matching scheme of this isophthalic toe board, please share your application scenario and required quantity with us, and we will provide detailed specifications and a quotation. You may also contact us for samples and technical support.

Operating Environment

  • This isophthalic resin toe board is a pultruded FRP structural profile, so it is suitable for both indoor and outdoor installation, for protecting wall bases, platform edges or walkway edges.
  • The isophthalic polyester resin system gives this profile better resistance to moisture and to splashes and spills of mild chemical media than standard orthophthalic resin, making it a practical choice for wet process areas, washdown areas and coastal or humid locations.
  • As a glass fiber reinforced composite, this toe board does not corrode like steel and does not require painting, so it maintains its function in wet, salt-laden or mildly corrosive environments.
  • Continuous service temperature and resistance to specific chemicals depend on the resin, the medium and the concentration involved; please share your on-site conditions with us, and we will confirm whether this isophthalic profile is the right grade for your project.