Product Category

Product details

Greenlogy TEC

FRP pultruded profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the outer reinforcement layer. After being fully impregnated, the material is heated, formed and cured in a metal die and pulled by a pultrusion machine to produce a new type of composite material with good physical properties, widely used in high-strength and long-span applications.

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Kick plateA*B*T
A*B*T
M2100*13*3.2 M型1.13.94*0.51*0.13 M型2.43
M3100*16*5 M型1.33.94*0.63*0.2 M型2.87
M4148*12*3 M型1.275.83*0.47*0.12 M型2.8
W1100*19*5 W型1.363.94*0.75*0.2 W型3
W2100*15*3.2 W型1.13.94*0.59*0.13 W型2.43
W3150*15*3.2 W型1.65.91*0.59*0.13 W型3.53

Markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation and entertainment

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy-metal protection and safety

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin type

Code

Resin type

Flame retardancy

Standard color

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Grass green, yellow, gray, orange

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

Vinyl ester type is economical with good performance, moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

General acid and alkali environments

Applications:

Greenlogy TEC pultruded FRP structural profiles are used across a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles deliver years of low-maintenance service in areas where steel, aluminum or timber members are traditionally specified. Today these profiles are often used in highly corrosive applications that would otherwise require stainless steel and other costly components.

Greenlogy TEC Profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638psi30000kgf/m²21092086

Tensile stress, transverse

D-638psi7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-63810^6psi2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-63810^6psi0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695psi30000

kgf/m²

21092086

Compressive stress, transverse

D-695psi15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-69510^6psi2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-69510^6psi1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790psi30000

kgf/m²

21092086

Flexural stress, transverse

D-790psi10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-79010^6psi1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-79010^6psi0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi2.8

10^6kgf/m²

1969

Shear modulus

---10^6psi0.45

10^6kgf/m²

316

Short-beam shear

D-2344psi4500

kgf/m²

3163813

Punch shear

D-732psi10000

kgf/m²

7030695

Notched cantilever beam impact, longitudinal

D-256ft.-lbs./in.25kg/m3.46

Notched cantilever beam impact, transverse

D-256ft.-lbs./in4kg/m0.55

Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495---45

24-hour water absorption

D-570% max0.45

Density

D-792lbs./in.³0.062-0.07

Coefficient of thermal expansion, longitudinal

D-69610^-6in./in./℃8

Flame retardancy

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame retardancy*

D-635---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, longitudinal

D-495

秒(s)

120

Dielectric strength, longitudinal

D-149kv./in.35

Dielectric strength, PF

D-149V/mil200

Dielectric constant, PF

D-150@60hz5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face

*Applies to ISOFR and VEFR only


Applications

Structural profiles - kick plates are commonly used in chemical platforms, wastewater treatment, marine engineering and power facilities and other corrosive environments, serving as edge protection and toe-board components, used together with FRP grating and pultruded profiles. To confirm suitability for your specific operating conditions, please contact us for detailed specifications and a quotation.

Selection guide

During selection, you can make an initial match from the A*B*T specifications based on the dimensions of the mounting surface, the required cross-sectional shape (such as M-shape) and load-bearing requirements. As specific parameters and customization needs are involved, we recommend providing drawings or operating conditions so that we can help recommend a suitable model. Please contact us for detailed specifications and a quotation.

Product advantages

This kick plate is pultruded from glass fiber reinforcement and resin, featuring corrosion resistance, light weight and high strength, electrical insulation, and ease of cutting and installation, making it suitable for high-humidity and chemical media environments. Different resin systems can meet various operating conditions. Please contact us for detailed specifications and a quotation.

Inquiry guidance

To learn about the available specifications, surface treatments and bulk supply information for structural profiles - kick plates, please provide us with your dimensions, quantity and operating environment. Please contact us for detailed specifications and a quotation; we will provide a targeted solution based on your requirements.