FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the wrapping reinforcement layer. After thorough impregnation, they are heated, formed, and cured in a metal mold and then pultruded by a pulling machine. They have good physical properties and are widely used in high-strength, large-span applications. 

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

I-beam

A*B*T1*T2


A*B*T1*T2


IB3215*32*6.4*40.510.59*1.26*0.25*0.161.12
IB38A30*38*3*30.531.18*1.5*0.12*0.121.17
IB45A45*9*180*125.41.77*0.35*7.09*0.4711.9
IB50A50*102*6.4*6.42.41.97*4.02*0.25*0.255.29
IB50B50*102*8*831.97*4.02*0.31*0.316.61
IB76A76*152*6.4*6.43.592.99*5.98*0.25*0.257.91
IB76B76*152*9.5*9.55.322.99*5.98*0.37*0.3711.73
IB102A102*203*9.5*9.57.24.02*7.99*0.37*0.3715.87
IB102B102*203*12.7*12.79.54.02*7.99*0.5*0.520.94
IB120120*240*12*1210.54.02*9.45*0.47*0.4723.15
IB127A127*254*9.5*9.595*10*0.37*0.3719.84
IB127B127*254*12.7*12.711.95*10*0.5*0.526.24
IB127C127*152*9.5*9.57.15*5.98*0.37*0.3715.65
IN127D127*152*12.7*12.79.25*5.98*0.5*0.520.28
IB152A152*305*9.5*9.510.75.98*12.01*0.37*0.3723.68
IB152B152*305*12.7*12.714.35.98*12.01*0.5*0.531.53

Application Markets 

  • Construction

  • Bridges & Highways

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gas

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Resistant to heavy metals

  • Long service life

  • Non-conductive, non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Standard colors

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Grass green, yellow, gray, orange

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

VEFR type, economical, with good performance and moderate resistance to acid, alkali and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

General acid and alkali environments

Applications:

  Greenlogy TEC pultruded FRP profiles are widely used in various scenarios, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. In areas where steel, aluminum or wood components have traditionally been specified, durable Greenlogy TEC profiles can provide years of low-maintenance service. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other expensive components.  

Greenlogy TEC Profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear strength

D-2344

psi

4500

kgf/m²

3163813

Punch shear strength

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round bars and square bars

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Maximum percentage

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volt/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

Structural profiles – I-beams are suitable for load-bearing and support locations requiring strength and span, such as platform walkways, trestles, equipment supports, handrail framing and structural frames in corrosive environments. Different resin systems and fiber lay-ups can be adapted to various service conditions; contact us for detailed specifications and a quotation.

Selection guidance

Selection should take into account load type, span, support conditions, service environment and connection method, on which basis section size and lengthwise requirements are determined. As service conditions vary considerably, we recommend providing your operating conditions so that we can help confirm a suitable model; contact us for detailed specifications and a quotation.

Product advantages

FRP I-beams are made from glass fiber reinforcement combined with resin, offering light weight and high strength, corrosion resistance, electrical insulation and non-magnetic properties, and ease of cutting and on-site fabrication, making them convenient substitutes where metal profiles tend to corrode. Specific performance varies with formulation and specification; contact us for detailed specifications and a quotation.

Inquiry guidance

To confirm section specifications, length, color, resin type or a matching connection solution, please provide drawings or service conditions and we will make recommendations accordingly. Contact us for detailed specifications and a quotation, and we can also discuss samples and bulk supply further.