Product Category

Structural Profiles - I-Beam (Isophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

    FRP pultruded profiles are a new type of composite material made with glass fiber as the reinforcement, resin as the binder, and glass fiber cloth as the wrapped reinforcing layer; after being fully impregnated, they are heated, formed and cured in a metal mold and then pulled by a pultrusion machine. They have good physical properties and are widely used in high-strength and long-span applications.   

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

I-shaped Profiles

A*B*T1*T2


A*B*T1*T2


IB32

15*32*6.4*4

0.51

9/16" x 5/4" x 1/4" x 3/16"

1.12

IB38A

30*38*3*3

0.53

19/16" x 3/2" x 1/8" x 1/8"

1.17

IB45A

45*9*180*12

5.4

7/4" x 3/8" x 7" x 1/2"

11.9

IB50A

50*102*6.4*6.4

2.4

2" x 4" x 1/4" x 1/4"

5.29

IB50B

50*102*8*8

3

2" x 4" x 5/16" x 5/16"

6.61

IB76A

76*152*6.4*6.4

3.59

3" x 6" x 1/4" x 1/4"

7.91

IB76B

76*152*9.5*9.5

5.32

3" x 6" x 3/8" x 3/8"

11.73

IB102A

102*203*9.5*9.5

7.2

4" x 8" x 3/8" x 3/8"

15.87

IB102B

102*203*12.7*12.7

9.5

4" x 8" x 1/2" x 1/2"

20.94

IB120

120*240*12*12

10.5

19/4" x 19/2" x 1/2" x 1/2"

23.15

IB127A

127*254*9.5*9.5

9

5" x 10" x 3/8" x 3/8"

19.84

IB127B

127*254*12.7*12.7

11.9

5" x 10" x 1/2" x 1/2"

26.24

IB127C

127*152*9.5*9.5

7.1

5" x 6" x 3/8" x 3/8"

15.65

IN127D

127*152*12.7*12.7

9.2

5" x 6" x 1/2" x 1/2"

20.28

IB152A

152*305*9.5*9.5

10.7

6" x 12" x 3/8" x 3/8"

23.68

IB152B

152*305*12.7*12.7

14.3

6" x 12" x 1/2" x 1/2"

31.53

Markets  

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and wastewater

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal safety

  • Long service life

  • Electrical and thermal insulation (non-conductive)

  • High strength-to-weight ratio

Raw material introduction — resin types

Designation

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR type, with excellent and moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

    Greenlogy TEC pultruded fiberglass structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.    

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

 Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% maximum

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 maximum

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Thanks to their lightweight, high-strength, corrosion-resistant and insulating properties, FRP I-beams are suitable for corrosive environments such as chemical platforms, offshore facilities, wastewater treatment plants, cooling towers and long-span walkways. Pultruded from glass fiber impregnated with resin, they maintain structural stability under damp, acid/alkali and salt-spray conditions.

Selection Guide

When selecting, please confirm the cross-section dimensions and resin system based on span, load type and support method; isophthalic resin is suitable for medium to high corrosion resistance requirements. For specific specifications and mechanical parameters, please provide your operating conditions and contact us for detailed specifications and selection advice.

Product Advantages

Compared with steel, FRP I-beams are lighter in weight, easier to transport and install, and offer excellent corrosion resistance, electrical insulation and non-magnetic properties. The pultrusion process ensures full fiber impregnation and continuous axial alignment, giving the profiles stable longitudinal strength. For specific performance data, please contact us for detailed technical information.

Inquiry Guide

For specifications, resin systems, custom lengths or bulk purchasing and other commercial terms, please contact us for detailed quotations and technical support. Our engineering team can provide selection assistance based on your project requirements.

Operating Environment

  • The I-beams are pultruded with isophthalic unsaturated polyester resin as the matrix and glass fiber as reinforcement, suitable for long-term use in corrosive environments such as damp conditions, acidic/alkaline media and salt spray, and can serve as load-bearing structures in chemical, wastewater treatment, marine engineering and similar applications.
  • The profiles resist rusting when used outdoors and are suitable for outdoor platforms, walkways and supports that are exposed to sun and rain over the long term; however, in environments with prolonged strong UV exposure, surface protection measures are recommended.
  • The I-beams are lightweight and high-strength, suitable for long-span, high-strength load-bearing conditions; when installed in indoor workshops, underground utility tunnels and other poorly ventilated locations, the applicability of the resin system should still be confirmed according to site conditions.
  • For the temperature range, medium concentration and installation load requirements of specific operating environments, please contact us to confirm so that we can recommend suitable specifications and resin types according to your conditions.