Structural Profiles - Hollow Section (Vinyl Ester Resin)
Product details
Greenlogy TEC
FRP pultruded profiles are made with glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the covering reinforcement layer. After thorough impregnation, they are heated, shaped, and cured in a metal mold and then pulled by a traction machine. This new type of composite material has good physical properties and is widely used in high-strength, long-span applications.
Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Hollow-core profile | A1*T1*A2*T2*B*T3 | A1*T1*A2*T2*B*T3 | ||
| 500*6*450*6*48.5*6 | 16.4 | 20" x 1/4" x 18" x 1/4" x 2" x 1/4" | 36.2 | |
| 500*6*450*6*48.5*9 | 18.5 | 20" x 1/4" x 18" x 1/4" x 2" x 3/8" | 40.8 | |
| 650*13*550*13*98.5*12 | 52.5 | 51/2" x 1/2" x 173/8" x 1/2" x 4" x 1/2" | 116 | |
| 725*4.5*675*4.5*45*4.5 | 17.9 | 57/2" x 3/16" x 53/2" x 3/16" x 7/4" x 3/16" | 39.5 |
Markets
Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Recreation
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistance
Low maintenance
Flame retardant
Low installation cost
Resistant to heavy metals
Long service life
Electrically and thermally non-conductive
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Harsh corrosive environments such as acids and alkalis |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type, economical, with good moderate resistance to acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP profiles from Greenlogy TEC are widely used in many applications, offering a unique combination of corrosion resistance, high strength, dimensional stability and light weight, together with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide many years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Mechanical properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of elasticity | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-beam shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod impact strength, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod impact strength, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | 25 max |
Flame resistance* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface
*Applies to ISOFR and VEFR only
Application Scenarios
Hollow-core structural profiles are suitable for industrial platforms, walkways, handrails, support structures and equipment frames that require high strength, long spans and corrosion resistance. Their light weight and high strength also make them a common choice for renovation projects that need reduced dead load or fast installation. Contact us and we will recommend suitable specifications based on your specific working conditions.
Selection Guide
When selecting, please consider factors such as load requirements, span, service environment (e.g. corrosive media, temperature) and installation method. You may provide cross-section dimensions, length and quantity, and we will help you match suitable profile specifications. Contact us for detailed specifications and a quotation.
Product Advantages
Made from glass fiber reinforcement combined with resin, this hollow-core profile offers light weight, high strength, corrosion resistance, electrical insulation and ease of processing, and maintains stable performance in a range of demanding environments. Its structural design balances load-bearing efficiency with weight control, making it easy to transport and install. Contact us to learn more about material properties and application cases.
Inquiry Guidance
For specific dimensions, weight, mechanical parameters or customized solutions for hollow-core structural profiles, please contact us directly. We can provide selection advice and commercial support based on your project requirements. Contact us for detailed specifications and a quotation.
Service Environment
- This hollow-core profile uses vinyl resin and is suitable for indoor and outdoor installations where moisture and water vapor are present.
- The vinyl resin matrix resists corrosive media, making this hollow-core profile suitable for chemical, wastewater and coastal environments where steel tends to deteriorate.
- Because the profile is made from glass fiber reinforcement combined with vinyl resin, it maintains structural integrity under various ambient temperatures without becoming brittle or losing shape.
- Typical locations of use include industrial plants, walkways, platforms and structural frames exposed long-term to weather, salt spray or process chemicals.