Structural Profiles - Hollow Board (Orthophthalic)
Product details
Greenlogy TEC
FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the adhesive, and glass fiber cloth as the covering reinforcement layer; after full impregnation, they are heated, formed and cured in a metal mold and pulled by a traction machine. With good physical properties, they are widely used in high-strength and long-span applications.
Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Hollow Profile | A1*T1*A2*T2*B*T3 | A1*T1*A2*T2*B*T3 | ||
| 500*6*450*6*48.5*6 | 16.4 | 20" x 1/4" x 18" x 1/4" x 2" x 1/4" | 36.2 | |
| 500*6*450*6*48.5*9 | 18.5 | 20" x 1/4" x 18" x 1/4" x 2" x 3/8" | 40.8 | |
| 650*13*550*13*98.5*12 | 52.5 | 51/2" x 1/2" x 173/8" x 1/2" x 4" x 1/2" | 116 | |
| 725*4.5*675*4.5*45*4.5 | 17.9 | 57/2" x 3/16" x 53/2" x 3/16" x 7/4" x 3/16" | 39.5 |
Application markets
Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Recreation
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistance
Low maintenance cost
Flame retardant
Low installation cost
Heavy-metal safety
Long service life
Electrical and thermal insulation
High strength-to-weight ratio
Introduction to raw materials — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 and above | ===== Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | ===== VEFR type is economical and offers good performance, with moderate acid, alkali and solvent resistance |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | ===== General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electrical insulation properties. Durable Greenlogy TEC profiles can provide many years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been specified. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Mechanical properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, longitudinal | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, transverse | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, longitudinal | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, transverse | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, longitudinal | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, transverse | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, longitudinal | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, transverse | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, longitudinal | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, transverse | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, longitudinal | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, transverse | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of elasticity | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short beam shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod impact strength, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod impact strength, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | Max. % | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max. 25 |
Combustibility* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face
*Applies only to ISOFR and VEFR
Application Scenarios
The orthophthalic hollow-profile structural section is suitable for load-bearing and support applications requiring high strength and larger spans, such as platform walkways, guardrail systems, frame structures and structural members in various corrosive environments. Its hollow cross-section reduces self-weight while maintaining structural stiffness, and facilitates on-site cutting and installation. For specific applicable working conditions, please contact us so that our technical staff can assess and recommend based on project conditions.
Selection Guidance
During selection, comprehensive consideration should be given to cross-section dimensions, wall thickness, span, load type and the corrosiveness of the service environment. In the table, the required specification can be matched using the designation format A1*T1*A2*T2*B*T3. The orthophthalic resin system offers good cost-effectiveness in general corrosive environments; if working conditions are special, you may discuss the choice of resin system with us. You are welcome to contact us for detailed specifications and selection advice.
Product Advantages
This profile uses glass fiber as reinforcement and resin as matrix, and is formed by impregnation, heated matched-die curing and continuous pultrusion. It has the common characteristics of composite materials such as light weight and high strength, corrosion resistance, and electrical insulation with no magnetism. The hollow structure helps improve flexural stiffness at the same section height, reducing material usage and installation load, and is suitable for structural locations with requirements on both self-weight and span.
Inquiry Guidance
If you need to know the specific specifications, dimensional tolerances, available lengths and commercial terms of the orthophthalic hollow-profile structural section, you are welcome to contact us. Please provide the required cross-section, quantity and service environment, and we will reply with detailed specifications and a quotation accordingly.
Service Environment
- This hollow-profile section is manufactured based on an orthophthalic resin system, so it is suitable for general indoor and outdoor service conditions where the structure is only intermittently exposed to moisture and chemical exposure is moderate, rather than continuously subjected to strong corrosion.
- Because this profile is a pultruded glass fiber reinforced composite material with glass fiber cloth reinforcement layers, it will not corrode like steel in humid factory environments, making it a practical choice for walkways, platforms and support frames in humid production areas and covered outdoor facilities.
- The hollow-profile section—a rectangular tube with internal ribs—is typically used as a structural member in moderate-temperature industrial environments; if the service environment involves concentrated acids, strong alkalis, continuous high temperatures or long-term UV exposure, buyers should confirm the resin grade and protection requirements before selection.
- For installations exposed to weather or washdown environments, fixing details and sealing of cut edges should be specified as part of the environmental assessment, because the long-term performance of the profile depends on whether the resin system matches the actual chemical, humidity and temperature conditions on site.