   FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the reinforcing body, resin as the matrix (adhesive), and glass fiber cloth as the covering reinforcement layer. After being fully impregnated, they are heated, formed, and cured in a metal mold, and then pulled by a pultrusion pulling machine. They have good physical properties and are widely used in high-strength, large-span applications.   

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

FL-A508*7*50.8*819.7

20" x 1/4" x 2" x 5/16"

43.4
FL-B635*12*101.6*1354.6

25" x 1/2" x 4" x 1/2"

120
FL-C498*4*50*49.4

20" x 3/16" x 2" x 3/16"

20.7

50*20*4*40.7

2" x 13/16" x 3/16" x 3/16"

1.54

55*31*3*30.6

9/4" x 5/4" x 1/8" x 1/8"

1.32

Market 

  • Construction

  • Bridges and Highways

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metal and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and Wastewater Treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal resistance

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio (high specific strength)

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type (isophthalic acid type) resin

Oxygen index 28 and above

VEFR type, economical, resistant to moderate acids, alkalis and solvents, with excellent performance

OFR-25

Orthophthalic type (phthalic acid type) resin

Oxygen index 28 and above

General acid and alkali environments

Applications:  

   Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide many years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been used. Today, these profiles are commonly used in highly corrosive applications where stainless steel and other costly components were once required.    

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact, longitudinal

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods  

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

Structural profiles – floor slabs (vinyl ester) are commonly used for platforms, walkways, trench covers, and support structures in corrosive environments such as chemical processing, electroplating, and wastewater treatment. Their high strength, light weight, and corrosion resistance also make them suitable for large-span, high-load industrial and marine engineering applications. For specific application conditions, please contact us for confirmation.

Selection Guide

When selecting, consider span, load, support spacing, and operating environment, and choose from different cross-sectional sizes and weight specifications such as FL-A, FL-B, and FL-C. For scenarios requiring special cutting, hole drilling, or splicing, we recommend providing drawings or application descriptions. Please contact us for detailed specifications and selection advice.

Product Advantages

This product uses glass fiber reinforcement and resin as the matrix, molded and pultruded to provide high strength, light weight, corrosion resistance, good insulation, and low maintenance costs. The vinyl ester material further enhances resistance to acids, alkalis, and chemical media, making it suitable for load-bearing floor slab applications exposed to harsh environments over the long term.

Inquiry Guide

For specific dimensions, weight, supply form, and commercial terms of structural profiles – floor slabs (vinyl ester), please contact us for detailed specifications and quotations. Please provide the required specifications, quantity, and operating environment, and we will match you with a suitable solution.