Greenlogy TEC

   FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the wrapping reinforcement layer; after thorough impregnation, the material is heated, formed, and cured in a metal mold and then pultruded by a pulling machine. With good physical properties, they are widely used in high-strength, long-span applications.   

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

FL-A508*7*50.8*819.7

20" x 1/4" x 2" x 5/16"

43.4
FL-B635*12*101.6*1354.6

25" x 1/2" x 4" x 1/2"

120
FL-C498*4*50*49.4

20" x 3/16" x 2" x 3/16"

20.7

50*20*4*40.7

2" x 13/16" x 3/16" x 3/16"

1.54

55*31*3*30.6

9/4" x 5/4" x 1/8" x 1/8"

1.32

Market 

  • Construction

  • Bridge and Highway

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metal and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and Wastewater Treatment

Features:

  • Corrosion Resistance

  • Low Maintenance

  • Flame retardant

  • Low installation cost

  • Heavy metal resistance

  • Long service life

  • Non-conductive, non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical product with good performance, moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:  

   Greenlogy TEC pultruded FRP structural profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles provide many years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been specified. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.    

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal (LW)

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse (CW)

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal (LW)

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse (CW)

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal (LW)

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse (CW)

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal (LW)

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse (CW)

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal (LW)

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse (CW)

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal (LW)

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse (CW)

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, longitudinal

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, transverse

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods  

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Max. %

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, lengthwise

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, lengthwise

D-495

秒(s)

120

Dielectric strength, lengthwise

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

Isophthalic structural profile floor panels are suitable for industrial platforms, walkways, trench covers and offshore facilities where high corrosion resistance is required. Their light weight, high strength and resistance to chemical attack make them widely used in the chemical, marine and wastewater treatment sectors.

Selection Guide

Selection should take into account load requirements, span, support spacing and the service environment. Profiles of different cross-sectional dimensions and thicknesses have different load-bearing capacities; we recommend consulting our technical team with your actual engineering conditions to obtain suitable specification recommendations.

Product Advantages

The isophthalic resin system gives the floor panels excellent corrosion resistance and water resistance, while glass fiber reinforcement ensures high strength and stiffness. The products are light in weight, easy to transport and install, and offer good electrical insulation and aging resistance.

Inquiry Guidance

For detailed specifications, technical parameters or customized solutions, please contact us for professional support and a quotation. We can provide selection advice and solutions based on your project requirements.

Service Environment

  • These isophthalic resin FRP floor profiles are pultruded glass fiber composites, suitable for indoor factory floors and outdoor walkways, platforms and stair treads, replacing steel grating in damp or wet environments.
  • The isophthalic resin matrix is selected to resist mildly corrosive media — splashes, salt-laden air and washdown conditions common in chemical, water treatment and coastal plants — rather than concentrated acids or strong solvents.
  • Because the pultruded profiles contain no steel core, they suit areas where conventional metal grating would require frequent recoating due to corrosion; their surface does not produce sparks and will not cause rust staining on surrounding structures.
  • Service temperature, chemical exposure and UV load vary with the installation environment; please contact Greenlogy TEC and provide the actual service conditions so that the appropriate resin grade, profile specification within the FL-A / FL-B / FL-C series, and fastening details can be confirmed.