Product Category

Structural Profiles - Flat Tube (Isophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP pultruded profiles are made of glass fiber reinforcement, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer; after full impregnation, they are heated, formed and cured in a metal mold and pulled out by a traction machine as a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Flat Tube

A*B*T1*T2


A*B*T1*T2


FT4444*25*3.2*3.20.8

7/4" x 1" x 1/8" x 1/8"

1.76
FT50A51*25*3*30.79

2" x 1" x 1/8" x 1/8"

1.74
FT50B51*25*6.4*6.41.54

2" x 1" x 1/4" x 1/4"

3.4
FT7676*35*3*61.55

3" x 11/8" x 1/8" x 1/4"

3.42
FT8080*60*5*52.5

25/8" x 19/8" x 3/16" x 3/16"

5.51
FT91A91*38*4*41.78

7/2" x 3/2" x 3/16" x 3/16"

3.92
FT112A112*91*6.4*6.44.46

9/2" x 7/2" x 1/4" x 1/4"

9.83
FT120120*45*3*32

19/4" x 7/4" x 1/8" x 1/8"

4.41
FT175175*50*9*97

55/8" x 2" x 3/8" x 3/8"

15.4

Markets 

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal resistant

  • Long service life

  • Electrical and thermal insulation

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardancy

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical, good performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

  Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, offering a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electrical insulation. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.  

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardancy

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Structural profiles—flat tubes (isophthalic)—are commonly used for load-bearing and support structures requiring strength and corrosion resistance, such as platform frames, handrail posts, walkway supports and equipment frames. The isophthalic resin system suits humid, acid/alkali or outdoor exposure environments and can replace some metal profiles in various operating conditions. For specific application scenarios and installation methods, please contact us.

Selection Guidance

When selecting, consider load direction, span, connection method and environmental media, and weigh the flat tube's cross-sectional dimensions, wall thickness and resin system. The dimension table on this page lists the cross-section and unit weight of each specification for preliminary comparison; actual load capacity and deflection must be confirmed through engineering design. For selection advice for a specific project, please contact us for detailed specifications and quotation.

Product Advantages

The pultrusion process arranges glass fibers continuously along the axial direction, giving the flat tube high axial strength and stiffness, along with the FRP characteristics of light weight, corrosion resistance, non-magnetic properties, insulation and ease of processing. The isophthalic resin system further improves resistance to humid and chemical environments and facilitates on-site cutting, drilling and bolted connections. For specific performance data, please contact us.

Inquiry Guidance

If you need to determine specifications, quantity, length or other customization requirements, please contact us for detailed specifications and quotation. Please provide the operating environment, load conditions and required cross-sectional dimensions, and we will provide selection advice and commercial terms accordingly.

Operating Environment

  • Pultruded FRP flat tubes made with isophthalic resin are suitable for indoor and outdoor use, including installations exposed to weathering and UV environments.
  • The isophthalic resin matrix enables FRP flat tubes to resist moisture, dampness, and splashing or immersion in water treatment and chemical process areas.
  • This structural profile is used in corrosive industrial environments where acids, alkalis, salts or chlorides attack conventional steel components.
  • Typical locations include chemical plants, water and wastewater treatment plants, cooling towers, coastal and marine structures, and other corrosive or high-humidity sites.