Product Category

Structural Profiles - Flat Panel (Orthophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

    Pultruded FRP profiles are made from glass fiber reinforcement as the raw material, resin as the binder, and glass fiber cloth as the covering reinforcement layer; after full impregnation, they are heated, formed and cured in a metal mold and pulled by a pulling machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Flat Sheet

Thickness × Width


Thickness × Width


FP32A

3.2*1000

6.18

1/8" x 39"

13.6

FP32B

3.2*1220

7.42

1/8" x 48"

16.4

FP40A

4*800

6.2

3/16" x 32"

13.7

FP40B

4*1200

9.19

3/16" x 48"

20.3

FP48

4.8*1000

9.3

3/16" x 39"

20.5

FP50A

5*440

4.25

3/16" x 17"

9.37

FP50B

5*1220

11.8

3/16" x 48"

26

FP64

6.4*1220

14.84

1/4" x 48"

32.7

FP95

9.5*1220

22.02

3/8" x 48"

48.6

FP127

12.7*1220

29.44

1/2" x 48"

64.9

FP160

16*1220

37.2

5/8" x 48"

82

FP190

19*1220

44.1

3/4" x 48"

97.2

FP254

25.4*1220

59

1" x 48"

130

Application markets 

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure and entertainment

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistant

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy-metal environment safe

  • Long service life

  • Electrical and thermal insulation

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 or above

Harsh acid, alkali and other corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 or above

An economical VEFR-type product with good performance, offering moderate acid, alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 or above

General acid and alkali environments

Applications:  

   Greenlogy TEC pultruded FRP profiles are used across a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal and electrical insulation properties. Durable Greenlogy TEC profiles deliver years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max 25

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = longitudinal, CW = transverse, PF = perpendicular to the laminate plane

*Applies only to ISOFR and VEFR


Applications

Structural Profiles – Flat Sheet (Orthophthalic) is commonly used in high-strength, long-span structural applications, such as platform walkways, trench covers, handrails and support frames, in industrial environments with requirements for corrosion resistance and load bearing. If your operating conditions involve acids, alkalis, moisture or outdoor exposure, please contact us and describe the service environment; we can help assess suitability.

Selection Guide

When selecting, we recommend first clarifying the sheet thickness and width, the span and support method, and the load type (concentrated or uniformly distributed) and corrosive media, then determining the specification together with the installation direction and fixing method. Different sizes correspond to different load-bearing performance; please contact us for detailed specifications and a quotation for specific thickness, width and load-bearing data.

Product Advantages

This sheet is a composite of glass fiber reinforcement and resin, formed by molding and pultrusion. It combines good physical properties with corrosion resistance, is relatively lightweight, and is easy to cut and install. Its surface is flat and its insulation is good, making it suitable for replacing some traditional metal sheets in corrosive or electromagnetically sensitive environments.

Inquiry Guide

To learn about the detailed specifications, dimensional customization, packaging and delivery methods of Structural Profiles – Flat Sheet (Orthophthalic), please contact us for detailed specifications and a quotation. Please provide thickness, width, length, quantity and service environment, and we will recommend a suitable solution accordingly.

Service Environment

  • This pultruded FRP flat sheet profile uses glass fiber as reinforcement and resin as binder, so it is suitable for both indoor installation and outdoor exposed environments with moisture and weather effects.
  • The resin system and glass fiber reinforcement make this flat sheet profile a practical choice for corrosive industrial surroundings, including chemical plants, wastewater treatment areas and coastal sites, where steel requires frequent replacement.
  • Because this flat sheet profile is produced by pulling resin-impregnated glass fiber through a heated metal die, it retains its shape in service and is typically used where high strength and larger spans are required.
  • To learn about temperature, humidity and chemical exposure limits for a specific project, please contact us for the complete parameter table of this flat sheet profile series; the dimensions shown in the table can be checked together with your operating conditions.