Structural Profiles - Flat Bar (Orthophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP pultruded profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the outer reinforcing layer. After thorough impregnation, the material is heated, formed and cured in a metal die and then pulled by a pultrusion machine, resulting in a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Riglet

Width × Thickness


Width × Thickness


FS19

19*6.4

0.25

3/4" x 1/4"

0.55

FS30A

30*3

0.18

19/16" x 1/8"

0.4

FS30B

30*6.4

0.37

19/16" x 1/4"

0.82

FS35

35*8

0.54

11/8" x 5/16"

1.19

FS38

38*5

0.37

3/2" x 3/16"

0.82

FS40A

40*8

0.62

25/16" x 5/16"

1.37

FS40B

40*10

0.79

25/16" x 3/8"

1.74

FS46B

46*6.4

0.58

29/16" x 1/4"

1.28

FS50A

50*2

0.25

2" x 1/16"

0.55

FS50B

50*4

0.38

2" x 3/16"

0.84

FS50C

50*6

0.59

2" x 1/4"

1.3

FS50D

50*8

0.76

2" x 5/16"

1.68

FS50E

50*15

1.43

2" x 9/16"

3.15

FS60A

60*2

0.24

19/8" x 1/16"

0.53

FS60B

60*4

0.48

19/8" x 3/16"

1.06

FS64

64*4.8

0.6

5/2" x 3/16"

1.32

FS70

70*4

0.55

11/4" x 3/16"

1.21

FS76

76*9.5

1.42

3" x 3/8"

3.13

FS100A

100*10

1.95

4" x 3/8"

4.3

FS100B

100*25

4.85

4" x 1"

10.7

FS102A

102*3.2

0.63

4" x 1/8"

1.39

FS102B

102*5

0.97

4" x 3/16"

2.4

FS102C

102*6.4

1.3

4" x 1/4"

2.87

FS120

120*10

2.4

19/4" x 3/8"

5.29

FS152A

152*10

2.92

6" x 3/8"

6.44

FS152B

152*20

5.9

6" x 13/16"

13

FS190

190*15

5.42

15/2" x 9/16"

12

FS280

280*10

5.32

11" x 3/8"

11.7

FS300

300*24

14.4

12" x 15/16"

31.8

FS355

355*5

3.5

14" x 3/16"

7.72

FS555

555*5

5.4

22" x 3/16"

11.9

FS751

751*5

7.2

30" x 3/16"

15.9

Markets

  • Construction

  • Bridges and Highways

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metals and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Recreation and Leisure

  • Telecommunications

  • Transportation

  • Water and Wastewater Treatment

Features:

  • Corrosion resistant

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal resistance

  • Long service life

  • Electrical and thermal insulation

  • High strength-to-weight ratio

Introduction to raw materials — resin types

Code

Resin type

Flame retardancy

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh acidic, alkaline and other corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR-type product with excellent performance and moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

 Applications:

   Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical Properties

ASTM

Unit

Value

Barcol Hardness

D-495

---

45

24-hour Water Absorption

D-570

Max. %

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion, LW

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel Test*

E-84

Flame Spread

Max. 25

Combustibility*

D-635

---

Non-combustible

Electrical Properties

ASTM

Unit

Value

Arc Resistance, LW

D-495

秒(s)

120

Dielectric Strength, LW

D-149

kv./in.

35

Dielectric Strength, PF

D-149

Volts/mil

200

Dielectric Constant, PF

D-150

@60hz

5

LW = Lengthwise, CW = Crosswise, PF = Perpendicular to Laminate Surface

*Only applicable to ISOFR and VEFR


Application Scenarios

Structural profile flat bar (orthophthalic) is widely used in chemical, power, marine engineering, construction and other fields for structural support, platform grating, guardrail systems and more. Its excellent corrosion resistance and high strength make it suitable for harsh environments such as high humidity and corrosive media.

Selection Guide

When selecting, consider factors such as load requirements, span, corrosive environment and installation method. Different specifications of flat bar have different load-bearing capacities; it is recommended to choose the appropriate size and thickness based on actual engineering requirements. Please contact us for detailed specifications and selection advice.

Product Advantages

This product uses an orthophthalic resin matrix and features excellent corrosion resistance, high strength and light weight. Its smooth surface is easy to clean and maintain, and it offers good insulation performance and a long service life, making it an ideal alternative to traditional metal materials.

Inquiry Guidance

For more product information, technical parameters or a quotation, please contact us at any time. Our professional team will provide customized solutions based on your needs. Please reach us via our website or by phone.

Operating Environment

  • These pultruded FRP flat bars (Riglet profiles) benefit from the corrosion resistance of the glass fiber reinforced resin matrix and are suitable for both indoor and outdoor structural applications.
  • The orthophthalic resin system provides durability in humid and chemically exposed environments, making the profiles suitable for industrial plants, chemical processing areas, and marine or coastal environments where moisture and salt spray are present.
  • FRP flat bar has a low thermal conductivity, performs reliably over a wide range of ambient temperatures, and does not corrode like steel, thereby extending service life in demanding environments.
  • For projects requiring specific environmental resistance or regulatory compliance, please provide us with your operating conditions so that we can confirm the appropriate configuration.