Product Category

Structural Profiles - Decking (Vinyl Ester)


Contact us for a quotation

Product details

Greenlogy TEC

   FRP pultruded profiles are a new type of composite material made from glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the covering reinforcement layer; after full impregnation, they are heated, formed, and cured in a metal mold and drawn by a haul-off machine. They have good physical properties and are widely used in high-strength, large-span applications.   

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Flooring Panels

A*T1*B*T2
A*T1*B*T2

305*6.4*47.5*6.48.5

12" x 1/4" x 15/8" x 1/4"

18.7

500*5*48.5*6.412

20" x 3/16" x 2" x 1/4"

26.5

500*5*40*59.8

20" x 3/16" x 25/16" x 3/16"

21.6

Application markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and wastewater

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Suitable for heavy metal environments

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR resin with excellent performance, suitable for medium acid, alkali and solvent environments

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

 Applications:  

   Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with non-conductive and non-thermal-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications where stainless steel and other expensive components were previously required.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

Excluding round rods and square rods  

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Combustibility*

D-635

---

Non-burning

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Vinyl structural profiles – decking are commonly used for platforms, walkways, trench covers and support structures with high corrosion resistance requirements, and are particularly suitable for damp, acid/alkali or salt-fog environments. For selection under specific operating conditions, please contact us for detailed specifications and a quotation.

Selection Guide

When selecting, consider span, load-bearing requirements, installation method and the type of corrosive medium, and use the profile's cross-sectional dimensions and unit weight for a preliminary match. For project-specific specification combinations and layout plans, please contact us for detailed specifications and a quotation.

Product Advantages

This decking is pultruded from glass fiber reinforcement and resin, offering light weight, high strength, corrosion resistance, insulation and dimensional stability, and is easy to cut and install. For available options of different resin systems and surface treatments, please contact us for detailed specifications and a quotation.

Inquiry Guidance

To confirm the decking model, length and accessories suitable for your project, please provide the operating environment and load-bearing requirements, and we will help verify the available range. Please contact us for detailed specifications and a quotation.

Operating Environment

  • These vinyl ester FRP flooring profiles are designed for indoor and outdoor structural applications, suitable for locations where moisture, humidity and weather exposure are persistent concerns.
  • The vinyl ester resin matrix resists corrosive media commonly found in chemical, marine and industrial processing environments, including splash zones and vapor zones.
  • Suitable for high-strength, long-span flooring applications in factories, platforms and walkways where steel would require frequent coating maintenance.
  • The operating temperature range and chemical resistance depend on the specific resin formulation; please contact Greenlogy TEC for environmental recommendations for your specific project.