Product Category

Structural Profiles - Deck (Orthophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

   FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the adhesive, and glass fiber cloth as the cladding reinforcement layer; after full impregnation, they are heated, formed, and cured in a metal mold and then pulled by a pulling machine. They have good physical properties and are widely used in high-strength and long-span applications.   

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Grating panels

A*T1*B*T2
A*T1*B*T2

305*6.4*47.5*6.48.5

12" x 1/4" x 15/8" x 1/4"

18.7

500*5*48.5*6.412

20" x 3/16" x 2" x 1/4"

26.5

500*5*40*59.8

20" x 3/16" x 25/16" x 3/16"

21.6

Application markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy-metal free

  • Long service life

  • Electrically and thermally non-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR product with good performance, offering moderate acid, alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

 Applications:  

   Greenlogy TEC pultruded FRP profiles are produced by Greenlogy TEC and are used in a wide range of applications, combining unique properties such as corrosion resistance, high strength, dimensional stability and light weight, together with thermal insulation and electrical non-conductivity. Durable Greenlogy TEC profiles deliver years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been specified. Today these profiles are commonly used in highly corrosive environments that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic modulus

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

Excluding round rods and square rods  

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Max. %

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = Lengthwise, CW = Crosswise, PF = Perpendicular to laminate face

*Applies only to ISOFR and VEFR


Application Scenarios

Structural profile - deck (orthophthalic) is suitable for platforms, walkways, trench covers and various load-bearing structures requiring strength and span, commonly found in corrosive environments such as chemical, power and water treatment. Selection varies considerably with different media, loads and span conditions; you are welcome to contact us with your operating conditions for suitable recommendations.

Selection Guide

When selecting, please consider span, load requirements, installation method and operating environment, and make a preliminary match against the section dimensions (A×T1×B×T2) and unit weight in the table above. If you need to balance strength, stiffness and weight, please contact us for detailed specifications and selection support.

Product Advantages

This deck profile is molded and pultruded from glass fiber reinforcement and an orthophthalic resin system, featuring light weight, high strength, corrosion resistance and good design flexibility, making it suitable for high-strength, long-span applications. Specific performance varies with section and resin system; please contact us to confirm suitability.

Inquiry Guide

For available section specifications, length options and commercial terms, please contact us for detailed specifications and a quotation. Please provide the required dimensions, quantity and operating environment, and we will respond accordingly.