Product Category

Structural Profiles - Curved Flat Bar (Orthophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

    FRP pultruded profiles are made from glass fiber reinforcement as the raw material, resin as the adhesive, and glass fiber cloth as the wrapping reinforcement layer. After thorough impregnation, they are heated, formed and cured in a metal mold and pulled by a pulling machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Corner Radius

Width × Thickness


Width × Thickness


FS50A50*3.20.29

2" x 1/8"

0.64
FS60A60*3.20.36

19/8" x 1/8"

0.79
FS7070*40.54

19" x 3/16"

1.19
FS90A90*3.20.54

7/2" x 1/8"

1.19
FS100100*3.20.6

4" x 1/8"

1.32
FS120120*30.7

19/4" x 1/8"

1.54

Application fields  

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistant

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Heavy metal resistant

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical with good performance, moderate resistance to acid, alkali and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

  Greenlogy TEC pultruded FRP structural profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and non-conductive properties. Where steel, aluminum or wood components have traditionally been specified, durable Greenlogy TEC profiles deliver years of low-maintenance operation. Today these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC Profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile Stress, Longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, Transverse

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, Longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, Transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, Longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, Transverse

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, Longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, Transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, Longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, Transverse

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, Longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, Transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic Modulus

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punching Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact, Longitudinal (LW)

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact, Transverse (CW)

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Maximum value %

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, longitudinal (LW)

D-696

10^-6in./in./℃

8

Flammability performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = longitudinal, CW = transverse, PF = perpendicular to the laminate surface

*Applicable to ISOFR and VEFR only


Applications

Curved flat bars are commonly used in structural parts that require a curved profile or edge reinforcement, such as platform handrails, walkway frames, equipment supports and decorative trim. Their orthophthalic resin system suits general industrial and outdoor environments; weathering and corrosion resistance should be assessed against actual service conditions. Contact us for detailed recommendations.

Selection Guide

When selecting, consider the arc radius, cross-section dimensions, load requirements and installation method to ensure compatibility with adjacent components. You may provide drawings or service conditions, and our technical team will help recommend suitable specifications. Contact us for detailed specifications and quotations.

Product Advantages

This profile is made from glass fiber reinforcement and an orthophthalic resin system through a pultrusion process. It offers light weight, high strength, corrosion resistance and electrical insulation, and its curved design facilitates streamlined structures. Compared with traditional metal materials, it is easier to cut and install, helping to reduce long-term maintenance costs.