Product Category

Structural Profiles - Curved Flat Bar (Isophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

    FRP profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the adhesive, and glass fiber cloth as the wrapping reinforcement layer; after thorough impregnation, they are heated, formed and cured in metal molds and then drawn by a haul-off machine. They have good physical properties and are widely used in high-strength, large-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Fillet radius

Width × Thickness


Width × Thickness


FS50A50*3.20.29

2" x 1/8"

0.64
FS60A60*3.20.36

19/8" x 1/8"

0.79
FS7070*40.54

19" x 3/16"

1.19
FS90A90*3.20.54

7/2" x 1/8"

1.19
FS100100*3.20.6

4" x 1/8"

1.32
FS120120*30.7

19/4" x 1/8"

1.54

Markets  

  • Construction

  • Bridges and Highways

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metals and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Recreational Facilities

  • Telecommunications

  • Transportation

  • Water and Wastewater Treatment

Product features:

  • Corrosion resistant

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Resistant to heavy metals

  • Long service life

  • Electrical and thermal insulation (non-conductive)

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

Type A VEFR, economical grade, good performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

  Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal and electrical insulation properties. In areas where steel, aluminum or wooden components have traditionally been used, durable Greenlogy TEC profiles provide years of low-maintenance service. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other expensive components.   

Greenlogy TEC Profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile Stress, Lengthwise

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, Crosswise

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, Lengthwise

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, Crosswise

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, Lengthwise

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, Crosswise

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, Lengthwise

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, Crosswise

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, Lengthwise

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, Crosswise

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, Lengthwise

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, Crosswise

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face

*Applies to ISOFR and VEFR only


Application Scenarios

Curved flat bars (isophthalic resin type) are commonly used in locations requiring curved-surface fitting and structural reinforcement, such as circumferential reinforcement of tanks, pipe supports, curved walkway frames, and edge finishing of handrails and platforms. The isophthalic resin system gives these profiles an advantage under operating conditions with higher corrosion resistance and weather resistance requirements, making them suitable for chemical, water treatment, marine and general industrial environments. Please confirm the specific applicable working conditions with us based on the media and load conditions.

Selection Guide

When selecting, we recommend first confirming the arc radius and the curvature of the mating surface, then determining the width and thickness according to the span and load requirements, and finally checking the hole positions and connectors according to the installation method (bolted fixing, bonding, or splicing with grating/profiles). The recommended specifications in the table are for general reference. If the existing specifications do not match your arc or load, please contact us for customization based on drawings and samples. Please contact us for detailed specifications and quotations.

Product Advantages

The combination of glass fiber reinforcement and isophthalic resin gives this profile the characteristics of light weight and high strength, corrosion resistance, electrical insulation and non-magnetic properties, and ease of cutting and installation, making it suitable for replacing some metal profiles to reduce dead weight and lower maintenance frequency. The pultrusion process ensures stable cross-sectional dimensions and continuous fiber distribution, and the curved structure makes stress distribution more uniform under load. Specific data such as the coefficient of thermal expansion and electrical insulation performance can be confirmed by requesting documentation.

Inquiry Guidance

If you need to confirm the specifications, resin system or matching connection solutions for curved flat bars, please provide information such as the service environment, arc radius, length and quantity, and we will assist in matching a suitable model. For commercial terms such as price, minimum order quantity and delivery time, please contact us for detailed specifications and quotations. Samples and technical support can also be discussed together.

Operating Environment

  • These FRP structural profiles are suitable for indoor and outdoor installation, including industrial plants, chemical processing areas and moist marine environments.
  • The isophthalic resin formulation offers stronger resistance to water and various corrosive media, making these profiles suitable for wet and chemical-exposure working conditions.
  • With glass fiber reinforcement and a protective glass fiber cloth surface layer, the profiles can withstand the ambient temperature variations common in industrial environments without losing structural integrity.
  • Typical applications include support structures in wastewater treatment facilities, cooling towers, and coastal or offshore platforms, where conventional materials may degrade.