Product Category

Structural Profiles - Channel (Vinyl Ester)


Contact us for a quotation

Product details

Greenlogy TEC

 FRP pultruded profiles are a new type of composite material made with glass fiber as the reinforcement, resin as the adhesive, and glass fiber cloth as a covering reinforcing layer; after full impregnation, they are heated, formed, and cured in a metal mold and pulled (pultruded) by a pulling machine. They have good physical properties and are widely used in high-strength and large-span applications.

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Channel

A*B*T1*T2


A*B*T1*T2


C2525*14*3*30.28

1" x 1/2" x 1/8" x 1/8"

0.62
C2626*18*3.2*3.20.3

1" x 11/16" x 1/8" x 1/8"

0.66
C3131*23*4*40.65

5/4" x 15/16" x 3/16" x 3/16"

1.43
C3232*13*3*30.25

5/4" x 1/2" x 1/8" x 1/8"

0.55
C3333*29*4*40.65

5/4" x 19/16" x 3/16" x 3/16"

1.43
C3636*30*4*40.68

3/2" x 5/4" x 3/16" x 3/16"

1.5
C4040*24*3.2*3.20.5

25/16" x 15/16" x 1/8" x 1/8"

1.1
C4545*28*6.4*6.41.07

7/4" x 9/8" x 1/4" x 1/4"

2.36
C5050*14*3.2*3.20.44

2" x 9/16" x 1/8" x 1/8"

0.97
C5252*50*6*61.63

33/16" x 2" x 1/4" x 1/4"

3.59
C7070*30*4.5*4.50.95

11/4" x 5/4" x 3/16" x 3/16"

2.09
C7575*35*5*51.37

3" x 11/8" x 3/16" x 3/16"

3.02
C76A76*22*6.4*6.41.31

3" x 7/8" x 1/4" x 1/4"

2.89
C76B76*38*6.4*6.41.7

3" x 3/2" x 1/4" x 1/4"

3.75
C8080*40*10*102.7

25/8" x 25/16" x 3/8" x 3/8"

5.95
C90A90*35*5*51.49

7/2" x 11/8" x 3/16" x 3/16"

3.28
C90B90*35*8*82.1

7/2" x 11/8" x 5/16" x 5/16"

4.63
C102A102*27*3.2*3.20.91

4" x 1" x 1/8" x 1/8"

2.01
C102B102*29*4.8*4.81.45

4" x 9/8" x 3/16" x 3/16"

3.2
C102C102*30*4*41.2

4" x 19/16" x 3/16" x 3/16"

2.65
C102E102*44*4.8*4.81.65

4" x 7/4" x 3/16" x 3/16"

3.64
C102F102*44*6.4*6.42.1

4" x 7/4" x 1/4" x 1/4"

4.63
C117117*85*5*52.7

37/8" x 27/8" x 3/16" x 3/16"

5.95
C120A120*25*5*51.52

19/4" x 1" x 3/16" x 3/16"

3.35
C120B120*30*5*51.62

19/4" x 19/16" x 3/16" x 3/16"

3.57
C120C120*40*5*51.81

19/4" x 25/16" x 3/16" x 3/16"

3.99
C145145*25*5*51.8

23/4" x 1" x 3/16" x 3/16"

3.97
C150A150*100*6.4*6.44.1

6" x 4" x 1/4" x 1/4"

9.04
C150B150*80*10*105.5

6" x 25/8" x 3/8" x 3/8"

12.13
C152A152*42*4.8*4.82.03

6" x 13/8" x 3/16" x 3/16"

4.48
C152B152*42*6.4*6.42.72

6" x 13/8" x 1/4" x 1/4"

6
C152C152*42*8*83.5

6" x 13/8" x 5/16" x 5/16"

7.72
C152D152*42*9.5*9.53.95

6" x 13/8" x 3/8" x 3/8"

8.71
C152E152*51*9.5*9.54.35

6" x 2" x 3/8" x 3/8"

9.59
C160160*48*8*83.7

25/4" x 15/8" x 5/16" x 5/16"

8.16
C203A203*56*6.4*6.43.68

8" x 9/4" x 1/4" x 1/4"

8.11
C203B203*56*9.5*9.55.34

8" x 9/4" x 3/8" x 3/8"

11.77
C203C203*102*12.7*12.79.2

8" x 4" x 1/2" x 1/2"

20.28
C210A210*55*5*52.95

33/4" x 9/4" x 3/16" x 3/16"

6.5
C210B210*80*5*53.42

33/4" x 25/8" x 3/16" x 3/16"

7.54
C210C210*85*5*53.52

33/4" x 27/8" x 3/16" x 3/16"

7.76
C240A240*72*8*85.7

19/2" x 11/4" x 5/16" x 5/16"

12.57
C240B240*115*5*54.4

19/2" x 9/2" x 3/16" x 3/16"

9.7
C254254*70*12.7*12.78.910" x 11/4" x 1/2" x 1/2"

19.62
C292292*70*12.7*12.79.8

23/2" x 11/4" x 1/2" x 1/2"

21.61
C300300*55*5*53.85

12" x 9/4" x 3/16" x 3/16"

8.49
C310A310*115*5*55.1

49/4" x 9/2" x 3/16" x 3/16"

11.24
C381381*90*10*1010.5

15" x 7/2" x 3/8" x 3/8"

23.15
C436436*90*10*1011.7

69/4" x 7/2" x 3/8" x 3/8"

25.79
C491491*90*12*1214.3

77/4" x 7/2" x 1/2" x 1/2"

31.53
C610610*76*6.4*6.49.2

24" x 3" x 1/4" x 1/4"

20.28
C902902*100*10*1020.6

71/2" x 4" x 3/8" x 3/8"

45.42
C970970*40*10*1019.9

153/4" x 25/16" x 3/8" x 3/8"

43.87

Markets  

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metal and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal resistance

  • Long service life

  • Non-conductive, non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin type

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR-grade product with excellent performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

  Greenlogy TEC pultruded FRP profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles offer years of low-maintenance service in areas traditionally specified for steel, aluminum or wood components. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel burn test*

E-84

Flame spread

25 max

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face

*Applies to ISOFR and VEFR only


Application Scenarios

Vinyl ester channel profiles are suitable for platforms, walkways, support frames and other applications with high corrosion resistance requirements, as well as humid or corrosive environments such as chemical plants and water treatment facilities. Their light weight and high strength make on-site cutting and installation convenient, and they can replace some traditional metal channels. For suitability for your specific operating conditions, please contact us to discuss.

Selection Guide

When selecting, consider span, load, support method and the type of corrosive medium to confirm the channel's cross-section dimensions and wall thickness. The vinyl ester resin system offers advantages in chemical resistance and is suitable for highly corrosive applications. For recommended specifications for a specific project, please contact us for technical support.

Product Advantages

Formed by pultrusion with glass fiber reinforcement and resin impregnation, the product features light weight, high strength, corrosion resistance, insulation and low maintenance. The surface can be covered with a glass fiber cloth reinforcement layer to improve overall mechanical performance and durability. For detailed performance data, please contact us.

Inquiry Guidance

For detailed specifications, dimensional tolerances, packaging and shipping methods for vinyl ester channel profiles, please contact us for detailed specifications and a quotation. We can provide selection advice and sample support based on your project requirements. We look forward to your inquiry.

Service Environment

  • Vinyl ester FRP channel profiles resist corrosion from acids, alkalis, salts and oxidizing media, making them suitable for chemical plants, wastewater treatment facilities and marine environments where steel tends to deteriorate.
  • These profiles perform reliably outdoors and in humid conditions, including exposure to moisture, salt spray and industrial atmospheres, without the need for additional protective coatings.
  • Vinyl ester FRP channel profiles have low thermal conductivity, which helps reduce thermal bridging in structural components and improve energy efficiency in both indoor and outdoor installations.
  • Typical applications include platforms and walkways in offshore and coastal environments, as well as support structures in pulp and paper mills, where continuous exposure to corrosive media requires durable and non-conductive materials.