Product Category

Structural Profiles - Channel (Orthophthalic)


Contact us for a quotation

Product details

Greenlogy TEC (Nantong Greenlogy TEC Electronic Technology Co., Ltd.)

 FRP pultruded profiles are a composite material made with glass fiber reinforcing material as the substrate, resin as the binder, and glass fiber cloth as the covering reinforcement layer. After thorough impregnation, they are heated, formed, and cured in a metal mold, and then pultruded by a pulling machine. They have good physical properties and are widely used in high-strength and large-span applications.

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Channel steel

A*B*T1*T2


A*B*T1*T2


C2525*14*3*30.28

1" x 1/2" x 1/8" x 1/8"

0.62
C2626*18*3.2*3.20.3

1" x 11/16" x 1/8" x 1/8"

0.66
C3131*23*4*40.65

5/4" x 15/16" x 3/16" x 3/16"

1.43
C3232*13*3*30.25

5/4" x 1/2" x 1/8" x 1/8"

0.55
C3333*29*4*40.65

5/4" x 19/16" x 3/16" x 3/16"

1.43
C3636*30*4*40.68

3/2" x 5/4" x 3/16" x 3/16"

1.5
C4040*24*3.2*3.20.5

25/16" x 15/16" x 1/8" x 1/8"

1.1
C4545*28*6.4*6.41.07

7/4" x 9/8" x 1/4" x 1/4"

2.36
C5050*14*3.2*3.20.44

2" x 9/16" x 1/8" x 1/8"

0.97
C5252*50*6*61.63

33/16" x 2" x 1/4" x 1/4"

3.59
C7070*30*4.5*4.50.95

11/4" x 5/4" x 3/16" x 3/16"

2.09
C7575*35*5*51.37

3" x 11/8" x 3/16" x 3/16"

3.02
C76A76*22*6.4*6.41.31

3" x 7/8" x 1/4" x 1/4"

2.89
C76B76*38*6.4*6.41.7

3" x 3/2" x 1/4" x 1/4"

3.75
C8080*40*10*102.7

25/8" x 25/16" x 3/8" x 3/8"

5.95
C90A90*35*5*51.49

7/2" x 11/8" x 3/16" x 3/16"

3.28
C90B90*35*8*82.1

7/2" x 11/8" x 5/16" x 5/16"

4.63
C102A102*27*3.2*3.20.91

4" x 1" x 1/8" x 1/8"

2.01
C102B102*29*4.8*4.81.45

4" x 9/8" x 3/16" x 3/16"

3.2
C102C102*30*4*41.2

4" x 19/16" x 3/16" x 3/16"

2.65
C102E102*44*4.8*4.81.65

4" x 7/4" x 3/16" x 3/16"

3.64
C102F102*44*6.4*6.42.1

4" x 7/4" x 1/4" x 1/4"

4.63
C117117*85*5*52.7

37/8" x 27/8" x 3/16" x 3/16"

5.95
C120A120*25*5*51.52

19/4" x 1" x 3/16" x 3/16"

3.35
C120B120*30*5*51.62

19/4" x 19/16" x 3/16" x 3/16"

3.57
C120C120*40*5*51.81

19/4" x 25/16" x 3/16" x 3/16"

3.99
C145145*25*5*51.8

23/4" x 1" x 3/16" x 3/16"

3.97
C150A150*100*6.4*6.44.1

6" x 4" x 1/4" x 1/4"

9.04
C150B150*80*10*105.5

6" x 25/8" x 3/8" x 3/8"

12.13
C152A152*42*4.8*4.82.03

6" x 13/8" x 3/16" x 3/16"

4.48
C152B152*42*6.4*6.42.72

6" x 13/8" x 1/4" x 1/4"

6
C152C152*42*8*83.5

6" x 13/8" x 5/16" x 5/16"

7.72
C152D152*42*9.5*9.53.95

6" x 13/8" x 3/8" x 3/8"

8.71
C152E152*51*9.5*9.54.35

6" x 2" x 3/8" x 3/8"

9.59
C160160*48*8*83.7

25/4" x 15/8" x 5/16" x 5/16"

8.16
C203A203*56*6.4*6.43.68

8" x 9/4" x 1/4" x 1/4"

8.11
C203B203*56*9.5*9.55.34

8" x 9/4" x 3/8" x 3/8"

11.77
C203C203*102*12.7*12.79.2

8" x 4" x 1/2" x 1/2"

20.28
C210A210*55*5*52.95

33/4" x 9/4" x 3/16" x 3/16"

6.5
C210B210*80*5*53.42

33/4" x 25/8" x 3/16" x 3/16"

7.54
C210C210*85*5*53.52

33/4" x 27/8" x 3/16" x 3/16"

7.76
C240A240*72*8*85.7

19/2" x 11/4" x 5/16" x 5/16"

12.57
C240B240*115*5*54.4

19/2" x 9/2" x 3/16" x 3/16"

9.7
C254254*70*12.7*12.78.910" x 11/4" x 1/2" x 1/2"

19.62
C292292*70*12.7*12.79.8

23/2" x 11/4" x 1/2" x 1/2"

21.61
C300300*55*5*53.85

12" x 9/4" x 3/16" x 3/16"

8.49
C310A310*115*5*55.1

49/4" x 9/2" x 3/16" x 3/16"

11.24
C381381*90*10*1010.5

15" x 7/2" x 3/8" x 3/8"

23.15
C436436*90*10*1011.7

69/4" x 7/2" x 3/8" x 3/8"

25.79
C491491*90*12*1214.3

77/4" x 7/2" x 1/2" x 1/2"

31.53
C610610*76*6.4*6.49.2

24" x 3" x 1/4" x 1/4"

20.28
C902902*100*10*1020.6

71/2" x 4" x 3/8" x 3/8"

45.42
C970970*40*10*1019.9

153/4" x 25/16" x 3/8" x 3/8"

43.87

Application markets  

  • Construction

  • Bridges and highways

  • Chemicals

  • Food and beverage

  • Manufacturing

  • Metal and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power generation

  • Pulp and paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and wastewater

Features:

  • Corrosion resistant

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Safe in heavy-metal environments

  • Long service life

  • Non-conductive and non-thermally conductive

  • High strength-to-weight ratio

Raw material overview — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Severe acid, alkali and other corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type, economical grade, with excellent resistance to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

  Greenlogy TEC pultruded FRP profiles are used across a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic modulus

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength (length direction)

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength (width direction)

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excluding round rods and square rods

Physical Properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Max. %

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion (LW)

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame resistance*

D-635

---

Non-combustible

Electrical Properties

ASTM

Unit

Value

Arc resistance (LW)

D-495

秒(s)

120

Dielectric strength (LW)

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Only applicable to ISOFR and VEFR


Application scenarios

Channel-section structural profiles are commonly used for load-bearing and support locations that require both strength and corrosion resistance, such as platform frames, walkway supports, equipment brackets and structural frames in corrosive environments including chemical plants and water treatment. Their cross-section facilitates combination and connection with other profiles, making them suitable for applications requiring long spans or high strength. Please confirm the specific applicable working conditions based on actual loads and environmental conditions.

Selection guidance

When selecting, it is recommended to first clarify the corrosion level of the service environment, load-bearing requirements and installation method, and then determine the cross-section specification, wall thickness and resin system accordingly; orthophthalic resin is suitable for general anti-corrosion working conditions, while highly corrosive or special media environments require separate evaluation. Listed above on this page are the channel section dimensions and unit weights, which can be used for preliminary comparison. For selection recommendations for specific projects, please contact us for detailed specifications and quotations.

Product advantages

This profile uses glass fiber as reinforcement and resin as matrix, and is formed by heated curing in a mold and continuous pultrusion. It features light weight and high strength, corrosion resistance, insulation and ease of processing, and is suitable for replacing some traditional metal profiles to reduce maintenance requirements. The surface can be covered or coated as required to suit different installation environments. Specific performance indicators are subject to the actual technical data supplied.

Inquiry guidance

For the complete specification table, weight parameters, available lengths and surface treatment options of the channel, please contact us for detailed specifications and quotations. Please provide the target cross-section dimensions, quantity, service environment and delivery requirements, and we will recommend a suitable solution accordingly and arrange further communication.

Service environment

  • These pultruded FRP channel profiles are composed of glass fiber reinforcement and an orthophthalic resin matrix. The finished channels can withstand moisture and washdown in damp indoor areas, as well as rain and humid outdoor air, and will not rust like steel channels.
  • Because the profile contains no steel core, the channels are suitable for chemical plants, wastewater treatment areas and coastal or offshore locations where acids, alkalis and salt-laden atmospheres attack conventional metal frames.
  • As a non-conductive structural profile, the channel is used for support frames near electrical equipment, cable trays and walkway stringers, where conductive metal profiles would require separate insulation treatment.
  • The glass fiber cloth reinforcement layers and the continuous pultrusion structure make it suitable both for sheltered factory interiors and for open-air structural projects; for the exact temperature, chemical exposure and load limits of a specific project, please provide application details and contact us.