Product Category

Structural Profiles - Channel (Isophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

 FRP profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the outer reinforcing layer; after thorough impregnation, they are heated, formed, and cured in a metal mold and then pultruded (drawn) by a pulling machine. They have good physical properties and are widely used in high-strength, large-span applications.

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Channel Steel

A*B*T1*T2


A*B*T1*T2


C2525*14*3*30.28

1" x 1/2" x 1/8" x 1/8"

0.62
C2626*18*3.2*3.20.3

1" x 11/16" x 1/8" x 1/8"

0.66
C3131*23*4*40.65

5/4" x 15/16" x 3/16" x 3/16"

1.43
C3232*13*3*30.25

5/4" x 1/2" x 1/8" x 1/8"

0.55
C3333*29*4*40.65

5/4" x 19/16" x 3/16" x 3/16"

1.43
C3636*30*4*40.68

3/2" x 5/4" x 3/16" x 3/16"

1.5
C4040*24*3.2*3.20.5

25/16" x 15/16" x 1/8" x 1/8"

1.1
C4545*28*6.4*6.41.07

7/4" x 9/8" x 1/4" x 1/4"

2.36
C5050*14*3.2*3.20.44

2" x 9/16" x 1/8" x 1/8"

0.97
C5252*50*6*61.63

33/16" x 2" x 1/4" x 1/4"

3.59
C7070*30*4.5*4.50.95

11/4" x 5/4" x 3/16" x 3/16"

2.09
C7575*35*5*51.37

3" x 11/8" x 3/16" x 3/16"

3.02
C76A76*22*6.4*6.41.31

3" x 7/8" x 1/4" x 1/4"

2.89
C76B76*38*6.4*6.41.7

3" x 3/2" x 1/4" x 1/4"

3.75
C8080*40*10*102.7

25/8" x 25/16" x 3/8" x 3/8"

5.95
C90A90*35*5*51.49

7/2" x 11/8" x 3/16" x 3/16"

3.28
C90B90*35*8*82.1

7/2" x 11/8" x 5/16" x 5/16"

4.63
C102A102*27*3.2*3.20.91

4" x 1" x 1/8" x 1/8"

2.01
C102B102*29*4.8*4.81.45

4" x 9/8" x 3/16" x 3/16"

3.2
C102C102*30*4*41.2

4" x 19/16" x 3/16" x 3/16"

2.65
C102E102*44*4.8*4.81.65

4" x 7/4" x 3/16" x 3/16"

3.64
C102F102*44*6.4*6.42.1

4" x 7/4" x 1/4" x 1/4"

4.63
C117117*85*5*52.7

37/8" x 27/8" x 3/16" x 3/16"

5.95
C120A120*25*5*51.52

19/4" x 1" x 3/16" x 3/16"

3.35
C120B120*30*5*51.62

19/4" x 19/16" x 3/16" x 3/16"

3.57
C120C120*40*5*51.81

19/4" x 25/16" x 3/16" x 3/16"

3.99
C145145*25*5*51.8

23/4" x 1" x 3/16" x 3/16"

3.97
C150A150*100*6.4*6.44.1

6" x 4" x 1/4" x 1/4"

9.04
C150B150*80*10*105.5

6" x 25/8" x 3/8" x 3/8"

12.13
C152A152*42*4.8*4.82.03

6" x 13/8" x 3/16" x 3/16"

4.48
C152B152*42*6.4*6.42.72

6" x 13/8" x 1/4" x 1/4"

6
C152C152*42*8*83.5

6" x 13/8" x 5/16" x 5/16"

7.72
C152D152*42*9.5*9.53.95

6" x 13/8" x 3/8" x 3/8"

8.71
C152E152*51*9.5*9.54.35

6" x 2" x 3/8" x 3/8"

9.59
C160160*48*8*83.7

25/4" x 15/8" x 5/16" x 5/16"

8.16
C203A203*56*6.4*6.43.68

8" x 9/4" x 1/4" x 1/4"

8.11
C203B203*56*9.5*9.55.34

8" x 9/4" x 3/8" x 3/8"

11.77
C203C203*102*12.7*12.79.2

8" x 4" x 1/2" x 1/2"

20.28
C210A210*55*5*52.95

33/4" x 9/4" x 3/16" x 3/16"

6.5
C210B210*80*5*53.42

33/4" x 25/8" x 3/16" x 3/16"

7.54
C210C210*85*5*53.52

33/4" x 27/8" x 3/16" x 3/16"

7.76
C240A240*72*8*85.7

19/2" x 11/4" x 5/16" x 5/16"

12.57
C240B240*115*5*54.4

19/2" x 9/2" x 3/16" x 3/16"

9.7
C254254*70*12.7*12.78.910" x 11/4" x 1/2" x 1/2"

19.62
C292292*70*12.7*12.79.8

23/2" x 11/4" x 1/2" x 1/2"

21.61
C300300*55*5*53.85

12" x 9/4" x 3/16" x 3/16"

8.49
C310A310*115*5*55.1

49/4" x 9/2" x 3/16" x 3/16"

11.24
C381381*90*10*1010.5

15" x 7/2" x 3/8" x 3/8"

23.15
C436436*90*10*1011.7

69/4" x 7/2" x 3/8" x 3/8"

25.79
C491491*90*12*1214.3

77/4" x 7/2" x 1/2" x 1/2"

31.53
C610610*76*6.4*6.49.2

24" x 3" x 1/4" x 1/4"

20.28
C902902*100*10*1020.6

71/2" x 4" x 3/8" x 3/8"

45.42
C970970*40*10*1019.9

153/4" x 25/16" x 3/8" x 3/8"

43.87

Markets  

  • Construction

  • Bridges & Highways

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gas [source reads 'Gsa' — apparent typo, please confirm]

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Heavy-metal resistant

  • Long service life

  • Electrical and thermal insulation

  • High specific strength

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 or above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 or above

An economical VEFR resin with good performance and resistance to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 or above

General acid and alkali environments

Applications: 

  Greenlogy TEC pultruded FRP profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductivity. Durable Greenlogy TEC profiles deliver years of low-maintenance service in areas traditionally specified for steel, aluminum or wood components. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic modulus

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excluding round bars and square bars

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max 25

Flame resistance*

D-635

---

Non-burning

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Structural profile – channel steel (isophthalic) is commonly used for load-bearing and support locations requiring strength and corrosion resistance, such as platform frames, walkway supports, handrail posts, equipment brackets, and structural members in corrosive environments including chemical and water treatment. The isophthalic resin system makes it suitable for contact with general corrosive media. Contact us to describe your service environment so we can confirm suitability.

Selection Guide

When selecting, please note the cross-section dimensions (A*B*T1*T2), unit weight and required load-bearing span, and confirm connection and hole requirements according to the installation method. The table lists multiple specifications for comparison. If you are unsure which one to choose, contact us with your operating conditions and we will help recommend a suitable specification.

Product Advantages

The channel steel is made of glass fiber reinforcement and isophthalic resin by pultrusion, offering the characteristics common to composites such as light weight, high strength, corrosion resistance, electrical insulation and non-magnetic properties, and is easy to cut and install on site. Compared with traditional metal channel steel, it reduces maintenance requirements in corrosive environments, making it suitable for projects with durability requirements.

Inquiry Guide

For detailed specifications, dimensional tolerances, supply forms and quotations, please contact us. Please state the required specification, quantity and service environment, and we will provide support as soon as possible.

Service Environment

  • Designed for FRP channel profile structural frames exposed to outdoor weathering, UV radiation and repeated wet-dry cycles, where the isophthalic resin matrix resists moisture absorption and surface degradation better than general-purpose resin systems.
  • Suitable for chemically corrosive plant areas handling acids, alkalis, salts and oxidizing splashes, because the pultruded glass fiber reinforcement and cured resin are selected for corrosion resistance, whereas structural steel requires continuous coating.
  • Maintains performance at ambient service temperatures typical of industrial walkways, platforms and support frames, retaining electrical insulation and non-sparking properties for areas near live equipment or where metal contact is a concern.