  Pultruded FRP grating is made with pultruded "I"-shaped and "T"-shaped profiles as load-bearing bars, solid tubes or rods as connecting rods, assembled through a specific assembly process, with gaps left on the panel surface.  

Property

Content

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Glass fiber

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction to Raw Materials 
Resin type

Code

Resin type

Flame retardancy

Recommended applications

MP-5

Phenolic type

Oxygen index up to approximately 80

Low toxicity and high flame retardancy; fire safety is extremely important in such applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh environments with strong corrosiveness such as acids and alkalis

VEFR-10

Vinyl ester type

Oxygen index 35 and above

Applications with high flame-retardant requirements and good acid and alkali resistance

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR economical grade, good performance, with moderate acid, alkali and solvent resistance

IFGR-30

Food grade (phenolic type)

Oxygen index 26

Mainly used in meat product and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical grade, no flame retardancy requirement

Selection of coarse glass fiber   

Code

Coarse sand type

Recommended applications

E

E-glass sand

For applications requiring high strength and high corrosion resistance

Select filler type

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing and corrosion-resistant applications

PR

No filler, pure resin

For high corrosion resistance applications

Sand surface

Smooth surface

Anti-slip grooved surface

Standard panel size:
1220mm,915mm-wide 3050mm,6100mm-length
Load-bearing bar: 38mm
Open area: 38%

Approx. weight (including three-strand hemp core): 14.2kg/m²

Line load (dimensions in mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Ultimate

(mm)

15030045075015003000

Load

4500.250.250.510.761.272.546288
6000.250.510.761.272.294.835021
9000.761.522.293.817.62---3353
12001.783.35.088.38------2503

Uniform load (dimensions in mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Ultimate

(mm)

4509501450240048509500

Load

450<0.250.250.250.511.272.5413713
6000.250.511.011.523.056.110297
9001.522.794.327.11------6881
12004.328.3812.7---------4099

Features:

  • Flame retardant

  • High flame retardancy

  • Low smoke and low toxicity emissions

  • High specific strength

  • Corrosion resistant

  • Low maintenance

  • Anti-slip

  • Electrically and thermally insulating

  • Easy to process

  • Impact resistant 

  • UV resistance

  • Maintenance-free

Installation and accessories  


Application scenarios

Pultruded grating T-3815 is suitable for platforms, walkways, trench covers and working surfaces that require both load-bearing capacity and corrosion resistance. It is commonly used in chemical, water treatment, power and marine engineering applications where corrosive media or humid environments are present. If you need to confirm suitability under specific media, temperature or load conditions, please contact us to discuss your operating details.

Selection guide

This product is assembled with pultruded "I" and "T" profiles as load-bearing bars and solid tubes or rods as connecting rods. When selecting, we recommend considering the load-bearing span, service environment and resin system (such as OFR, IFR, VEFR or phenolic type) together. Different resin types offer different flame-retardant and corrosion-resistant performance. Please provide your operating conditions and we will help recommend a suitable configuration.

Product advantages

Compared with traditional metal grating, pultruded grating features light weight, high strength, corrosion resistance and maintenance-free operation. It resists rusting during long-term use and is easy to cut and install on site. Its longitudinal load-bearing bar structure gives the panel good load-bearing capacity in the span direction, making it suitable for locations requiring frequent maintenance access or long-term exposure to corrosive environments.

Inquiry guidance

To learn about the detailed specifications, resin system options and commercial terms of pultruded grating T-3815, please contact us for detailed specifications and a quotation. Please provide your service environment, load requirements and dimensional needs, and we will provide a targeted solution and supply information accordingly.