Product details
Greenlogy TEC
Pultruded FRP grating is made from pultruded "I"-shaped and "T"-shaped profiles as load-bearing bars, with solid tubes or rods as connecting rods, assembled through a specific assembly process, and the panel surface has a certain gap.
Name | Content | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Glass fiber | 65% | E |
Filler | 8% | ATH,PR |
Other | 2% | --- |
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index up to about 80 | Low toxicity and high flame retardancy, for applications with high fire safety requirements |
VEFR-25 | Vinyl type | Oxygen index 28 and above | Harsh environments with strong corrosiveness such as acids and alkalis |
VEFR-10 | Vinyl type | Oxygen index 35 and above | Strong acids and strong alkalis with high flame retardant requirements, and applications with good service conditions |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR economical grade, good performance, moderate acid/alkali and solvent resistance |
IFGR-30 | Benzene grade, food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
OCR | Orthophthalic type | Oxygen index below 28 | OFR-25 economical grade, no flame-retardant requirement |
Coarse glass fiber selection
Code | Coarse sand type | Recommended applications |
E | Alkali-free sand | For applications requiring high strength and high corrosion resistance |
Selected filler type
Code | Filler type | Recommended applications |
|---|---|---|
ATH | Aluminum hydroxide | Flame-retardant, smoke-suppressing, corrosion-resistant applications |
PR | No filler, pure resin | For high corrosion resistance applications |
Standard panel dimensions:
1220 mm, 915 mm wide; 3050 mm, 6100 mm long
Load-bearing flat bar: 25 mm
Open area: 38%
Approximate weight (including three-core strand): 11.8 kg/m²
Pad load (unit: mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit value |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.71 | 1.02 | 1.73 | 3.45 | 6.91 | --- | 8600 |
| 600 | 1.55 | 2.34 | 3.89 | 7.75 | --- | --- | 6427 |
| 900 | 4.83 | 7.21 | --- | --- | --- | --- | 4180 |
| 1200 | 10.8 | --- | --- | --- | --- | --- | 3018 |
Uniform load (unit: mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit value |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 450 | 0.66 | 1.3 | 2.62 | 5 | 6.53 | --- | 37624 |
| 600 | 1.96 | 3.89 | 7.77 | --- | --- | --- | 21087 |
| 900 | 9.02 | --- | --- | --- | --- | --- | 9158 |
| 1200 | 6.6 | 13 | --- | --- | --- | --- | 9920 |
Features:
Flame retardant
High flame retardancy
Low smoke and low toxicity emissions
High strength-to-weight ratio
Corrosion resistant
Low maintenance
Anti-slip
Electrical and thermal non-conductive
Easy to fabricate
Impact resistance
UV resistance
Maintenance-free
Installation and accessories
Application scenarios
Pultruded grating T-3810 is commonly used for industrial platforms, walkways, trench covers, stair treads and equipment operating surfaces that require load-bearing capacity and corrosion resistance. Because pultruded profiles are used as load-bearing bars, it is suitable for environments requiring long spans, light weight, high strength and resistance to chemical media, such as chemical processing, water treatment, electroplating and marine engineering. To confirm suitability for specific media and operating conditions, please contact us for detailed specifications and selection advice.
Selection guide
Selection should take into account the resin system, grating thickness, load-bearing bar spacing, load-bearing direction and installation support conditions. Different resin types differ in flame retardancy and corrosion resistance, and the matching resin grade should be selected according to the actual environment. We can provide selection guidance based on your load, span and media conditions; please contact us to discuss your specific requirements.
Product advantages
Pultruded grating is assembled from pultruded I/T profiles as load-bearing bars together with solid tubes or rods as connecting rods, combining high specific strength, light weight, corrosion resistance and ease of cutting and installation. Compared with conventional metal grating, it is insulating, non-magnetic and low in maintenance cost, making it suitable for long-term exposure to damp or corrosive environments. For more details on material composition and structural advantages, please contact us.
Inquiry guidance
For detailed specifications, load parameters, resin options and custom solutions for pultruded grating T-3810, please contact us. Please provide your operating environment, dimensional requirements and load requirements, and we will provide a quotation and technical support accordingly. All commercial terms are subject to the inquiry communication confirmed by both parties.
Operating environment
- Pultruded FRP grating T-3810 is constructed from pultruded "I"-shaped or "T"-shaped profiles as load-bearing bars and solid tubes or rods as connecting rods, and is suitable for indoor and outdoor industrial platforms, walkways and tread boards.
- The vinyl ester resin VEFR-25 used in this grating has an oxygen index of 28 or above, supporting use in damp or mildly corrosive environments with moisture and chemical exposure.
- For fire-safety-critical locations with low-toxicity requirements, the MP-5 phenolic resin option can provide high flame retardancy, making the grating suitable for enclosed or high-risk process areas.
- Please contact us for the complete parameter list to confirm resin selection and configuration according to your specific temperature, humidity and chemical exposure conditions.